MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos H07G-00 Polypropylene Homopolymer
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Grade H07G-00 is a barefoot polypropylene homopolymer designed for cast film applications and flexible packaging. This grade has good optical properties and consistent processing. This grade meets the requirements of the U.S. Food and Drug Administration specified in 21 CFR 177.1520.

Key Words: Good optical properties and consistent processing
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.909 g/cc0.0328 lb/in³ASTM D792
Melt Flow 7.53 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.53 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 102102ASTM D785
Tensile Strength at Break 18.79 MPa2725 psi2 in/min; ASTM D638
Tensile Strength, Yield 36.0 MPa5220 psi2 in/min; ASTM D638
Elongation at Break 160 %160 %2 in/min; ASTM D638
Elongation at Yield 11 %11 %2 in/min; ASTM D638
Flexural Modulus, 1% Secant 1529 MPa221700 psiASTM D790A
Izod Impact, Notched 0.283 J/cm0.530 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 92.8 °C199 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 25 %
@Thickness 1.30 mm
25 %
@Thickness 0.0512 in
75% Diffuse Transmission; ASTM D1003
Gloss 93 %93 %60° Angle; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
ProcessFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem H 401 Cast Film Extrusion Polypropylene
ExxonMobil PP1364E2 Polypropylene Homopolymer
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 0% Cold Reduction
AKG Polymers Vision PP PPH Jazz0502dark Polypropylene Homopolymer Compound
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 15% Cold Reduction

PINEOS917 / 171732

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.