MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3A Composites Core Materials AIREX® C70.48 Universal Structural Foam
Categories: Other Engineering Material; Composite Core Material; Polymer

Material Notes: AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible water absorption, and provides an excellent resistance to chemicals. A fine cell structure offers an excellent bonding surface. Compatible with most resins and manufacturing processes AIREX® C70 is ideally suited as a core material for a wide variety of lightweight sandwich structures subjected to both static and dynamic loads.

Characteristics

  • outstanding strength and stiffness to weight ratios
  • Good impact strength
  • Low resin absorption
  • High fatigue resistance
  • Good fire performance (self-extinguishing)
  • Sound and thermal insulation
  • Good styrene resistance
Applications
  • Marine: Hulls, decks, bulkheads, superstructures, interiors
  • Road and Rail: Roof panels, interiors, floors, doors, partition walls, side skirts, front-ends
  • Aircraft: Interiors, radomes, galley carts, general aviation (fuselage and wing)
  • Recreation: Skis, snowboards, surfboards, wakeboards, canoes, kayaks
  • Industrial: Tooling, tanks, ductwork, containers, covers
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.0480 g/cc0.00173 lb/in³average; ISO 845
     0.0430 - 0.0550 g/cc0.00155 - 0.00199 lb/in³typical range; ISO 845
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength >= 0.800 MPa>= 116 psiin the plane; ISO 527 1-2
     0.950 MPa138 psiaverage; in the plane; ISO 527 1-2
    Elongation at Break >= 8.0 %>= 8.0 %shear; ISO 1922
     10 %10 %average; shear; ISO 1922
    Tensile Modulus >= 0.0280 GPa>= 4.06 ksiin the plane; ISO 527 1-2
     0.0350 GPa5.08 ksiaverage; in the plane; ISO 527 1-2
    Compressive Strength >= 0.500 MPa>= 72.5 psiperpendicular to plane; ISO 844
     0.600 MPa87.0 psiaverage; perpendicular to plane; ISO 844
    Compressive Modulus >= 0.0350 GPa>= 5.08 ksiperpendicular to plane; DIN 53421
     0.0480 GPa6.96 ksiaverage; perpendicular to plane; DIN 53421
    Shear Modulus >= 0.0140 GPa>= 2.03 ksiASTM C393
     0.0160 GPa2.32 ksiaverage; ASTM C393
    Shear Strength >= 0.500 MPa>= 72.5 psiISO 1922
     0.550 MPa79.8 psiaverage; ISO 1922
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity 0.0310 W/m-K0.215 BTU-in/hr-ft²-°FISO 8301
     
    Descriptive Properties
    Colorviolet

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    3A Composites Core Materials AIREX® C70.200 Universal Structural Foam
    3A Composites Core Materials AIREX® C70.75 Universal Structural Foam
    3A Composites Core Materials AIREX® C70.55 Universal Structural Foam
    3A Composites Core Materials AIREX® C51.60 Industrial Processing Foam
    3A Composites Core Materials AIREX® T92.100 Easy Processing Structural Foam

    PZ3AC006 / 108495

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.