MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Syensqo (Solvay Specialty Polymers) Ixef® 2060 Polyarylamide (PARA)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyarylamide (PAA); Polyarylamide, Glass Fiber Filled

Material Notes: Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent properties in the transverse direction. - Black: Ixef 2060/9008 - Custom Colorable

Injection Notes: Hot Runners: 250°C to 260°C (482°F to 500°F) Injection Pressure: rapid Drying The material as supplied is ready for molding without drying. However, If the bags have been open for longer than 24 hours, the material needs to be dried. When using a desiccant air dryer with dew point of -28°C (-18°F) or lower, these guidelines can be followed: 0.5-1.5 hour at 120°C (248°F), 1-3 hours at 100°C (212°F), or 1-7 hours at 80°C (176°F). Injection Molding IXEF 2060 compound can be readily injection molded in most screw injection molding machines. A general purpose screw is recommended, with minimum back pressure. The measured melt temperature should be between 265°C to 275°C (477-495°F), and the barrel temperatures should be around 250°C to 260°C (482°F to 500°F) in the rear zone, gradually increasing to 260°C to 290°C (500°F to 554°F) in the front zone. If hot runners are used, they should be set to 250°C to 260°C (482°F to 500°F). To maximize crystallinity, the temperature of the mold cavity surface must be held between 120°C to 140°C (248°F and 284°F). Molding at a lower temperature will produce articles that may warp, have poor surface appearance, and have a greater tendency to creep. Set injection pressure to give rapid injection. Adjust holding pressure and hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled (95%-99%).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³ISO 1183
Filler Content 55 %55 %Glass Fiber
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.2 %1.2 %65% RH
Linear Mold Shrinkage, Flow 0.0015 - 0.0025 cm/cm0.0015 - 0.0025 in/in
Linear Mold Shrinkage, Transverse 0.0025 - 0.0045 cm/cm0.0025 - 0.0045 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 80.0 MPa11600 psiWeldline; ISO 527-2
 180 MPa26100 psiISO 527-2
Elongation at Break 1.5 %1.5 %ISO 527-2
Tensile Modulus 19.0 GPa2760 ksiISO 527-2
Flexural Strength 270 MPa39200 psiISO 178
Flexural Modulus 18.0 GPa2610 ksiISO 178
Charpy Impact Unnotched 2.70 J/cm²12.8 ft-lb/in²ISO 179
Charpy Impact, Notched 0.440 J/cm²2.09 ft-lb/in²ISO 179
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 250 - 260 °C482 - 500 °F
Front Barrel Temperature 260 - 290 °C500 - 554 °F
Melt Temperature 247 - 257 °C477 - 495 °F
Mold Temperature 120 - 140 °C248 - 284 °F
Drying Temperature 120 °C
@Time 1800 - 5400 sec
248 °F
@Time 0.500 - 1.50 hour
 
Descriptive Properties
AppearanceBlack
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
FeaturesGood Chemical Resistance
 Good Creep Resistance
 Good Dimensional Stability
 High Flow
 High Strength
 Low Moisture Absorption
 Low Warpage
 Outstanding Surface Finish
 Ultra High Stiffness
FormsPellets
Processing MethodInjection Molding
RoHS ComplianceRoHS Compliant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik DYNACOLL® 7130 Copolyester
Covestro DESMOPHEN® 1200 BA Polyurethane
Evonik DYNACOLL® 7380 Copolyester
Syensqo (Solvay Specialty Polymers) Ixef® 1023 Polyarylamide (PARA)
Syensqo (Solvay Specialty Polymers) Ixef® 1028 Polyarylamide (PARA)

PSOL8Y898 / 107682

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.