MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled; Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability

Features: Good Dimensional stability; Good Processability; Heat Stabilized; Good Impact Resistance; Good Toughness; High Strength

Processing Method: Injection Molding

Forms: Pellets

Additive: Heat Stabilizer

Automotive Specifications: Chrysler MS-DB41 CPN1987 Color: BK001 Black; Ford ESA-M4D189-A; GM GMP.PA66.057

Information Provided by Teknor Apex

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 1.2 %1.2 %24 hr; ASTM D750
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 235 °C
20 g/10 min
@Load 4.76 lb,
Temperature 455 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 96.5 MPa14000 psiASTM D638
Elongation at Break 7.0 %7.0 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Flexural Strength 134 MPa19500 psiASTM D790
Flexural Modulus 3.79 GPa550 ksiASTM D790
Izod Impact, Notched  0.694 J/cm
@Temperature -40.0 °C
1.30 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 1.33 J/cm
@Temperature 22.8 °C
2.50 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Strength 11.0 kV/mm
@Thickness 3.00 mm
280 kV/in
@Thickness 0.118 in
ASTM D149
Comparative Tracking Index 500 V500 VUL 746
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 215 °C419 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 0.810 mm
HB
@Thickness 0.0319 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 241 - 257 °C465 - 495 °F
Middle Barrel Temperature 263 - 274 °C505 - 525 °F
Front Barrel Temperature 263 - 282 °C505 - 540 °F
Nozzle Temperature 263 - 279 °C505 - 535 °F
Melt Temperature 257 °C495 °F
 263 - 279 °C505 - 535 °FProcessing Temperature
Mold Temperature 60.0 - 93.3 °C140 - 200 °F
Drying Temperature 79.4 °C175 °F
Moisture Content 0.20 %0.20 %
Screw Speed 60 - 120 rpm60 - 120 rpm
 
Descriptive Properties
AppearanceBlack; Natural Color
Suggested Regrind, max25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylon® N1013STHL Nylon 6/6 (Cond)
AISI 1045 Steel, cold drawn, annealed, 19-32 mm (0.75-1.25 in) round
Teknor Apex Chemlon® 113 GH Nylon 66, 13% Short Glass Fiber Reinforced
Celanese Zytel® 80G14AHS BK099 PA66-IGF14
Celanese Zytel® 80G14A NC010A PA66-IGF14

PTEKNO432 / 128609

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.