MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Iran Petrochemical (PCC) SH-0150 Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: SH - 0150 ABS extrusion grade has been formulated to provide excellent mechanical properties,extrusion stability, vacuum formability and chemical resistance. It is a high flow extrusion grade with high impact strength at ambient temperature and considerable impact strength at low temperatures. This grade has a wide processing window.

Applications: parts with significant impact resistance, general sheets.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
Melt Flow 1.1 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.1 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 106106ASTM D785
Tensile Strength, Yield 44.1 MPa6400 psiASTM D638
Flexural Yield Strength 63.7 MPa9250 psiASTM D790
Flexural Modulus 2.21 GPa321 ksiASTM D790
Izod Impact, Notched (ISO) 28.0 kJ/m²13.3 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 101 °C214 °FASTM D1525
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) SD-0150 Acrylonitrile Butadiene Styrene
Chi Mei Polylac® PA-757 ABS
Iran Petrochemical (PCC) SBR-1500 Styrene Butadiene Rubber
Iran Petrochemical (PCC) SV-0157 Acrylonitrile Butadiene Styrene
Iran Petrochemical (PCC) S 30 S Polypropylene

PIPC356 / 149790

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.