MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom HRC 183D G84014 Polypropylene with 30% Talc Filler  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Talc Filler

Material Notes: Hostacom HRC 183D G84014 is a 30% talc filled PP homopolymer, with good hot water resistance, low discoloration under hot water/steam immersion and good detergent resistance. The product is also available as a customized color matched, pellet form. This grade is delivered in G84014 color version.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183-1A
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 33.0 MPa4790 psiISO 527-1,-2
Elongation at Break 8.0 %8.0 %ISO 527-1,-2
Tensile Modulus 3.40 GPa493 ksiISO 527-1,-2
Flexural Modulus 3.60 GPa522 ksiTech.A; ISO 178/A1
Charpy Impact Unnotched 2.80 J/cm²
@Temperature 23.0 °C
13.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eU
Charpy Impact, Notched 0.220 J/cm²
@Temperature 23.0 °C
1.05 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C163 °Funannealed; ISO 75A-1,-2
Vicat Softening Point 100 °C212 °FB50; ISO 306
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type S2 Tool Steel, austenitized 845°C (1550°F), brine quenched to 15 HRC
AISI Type 651 (19-9) Stainless Steel cold rolled and stress relieved, 35 HRC hardness
AISI Type S2 Tool Steel, austenitized 845°C (1550°F), brine quenched to 35 HRC
AISI Type S2 Tool Steel, austenitized 845°C (1550°F), brine quenched to 55 HRC
AISI Type S5 Tool Steel, austenitized 855-870°C (1575-1600°F), oil quenched to 45 HRC

PEQT7993 / 219629

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.