MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vibrantz Technologies IX 2405 Dental Glass
Categories: Ceramic; Glass

Material Notes: Glass Type: Sr-Al-B-Si
Typical Application: Phase Separated Glass Filler

Ferro's Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro also manufactures custom formulations to meet specific customer requirements. All powders are manufactured to tight composition, physical properties, and particle size distribution while maintaining low levels of heavy metal (Fe, Pb) contamination. Ferro IX 2405 is under license by the American Dental Association.

Information provided by Ferro Corporation

Ferro Corporation is now a part of Vibrantz Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.81 g/cc0.102 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.50 µm/m-°C
@Temperature 25.0 - 260 °C
3.06 µin/in-°F
@Temperature 77.0 - 500 °F
Softening Point 813 °C1500 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.551.55
 
Descriptive Properties
Purity LevelsCopper < 20 ppm
 Iron < 50 ppm
 Lead < 50 ppm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade
Vibrantz Technologies IX 1944 Dental Glass
Vibrantz Technologies EG 2810 Dental Glass
Vibrantz Technologies EG 2738 Dental Glass
Vibrantz Technologies IX 2693 Dental Glass

CFERR09 / 823

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.