MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ineos Nova Zylar® 94-580-A High Performance Styrenic, Acrylic Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Polystyrene (PS)

Material Notes: Excellent heat distortion temperature, High clarity, strength and toughness, Enhanced mold release

Applications: Industrial covers and housings, Paper towel dispenser covers, Appliance parts

Injection Speed: Slow to Moderate

Characteristic property data is based on tests of clear or crystal material. Colored material may differ in some properties. All molded samples were an 1/8 thick unless noted.

General information about ZYLAR®: ZYLAR® acrylic copolymers are The Clear Alternative to polycarbonate, PETG, impact acrylic and clear ABS for applications that demand clarity and toughness and enhanced processing productivity. ZYLAR is a cost effective alternative in injection molding applications, with over 15 years of proven performance.

ZYLAR has proven performance in a variety of applications, including medical, floor care, appliances, consumer goods, office accessories and supplies, pens and mechanical pencils, commercial paper towel dispensers, point of purchase displays, cosmetics packaging, toys, electronics packaging, housewares, consumer & industrial, and other applications.

ZYLAR® acrylic copolymers provide value through enhanced performance, manufacturing productivity, ease of processing, and potential for capital avoidance through utilization of existing (styrenics) equipment and tooling.

Performance Attributes:

  • Crisp clarity
  • Outstanding practical toughness and ductility
  • Balance of toughness and clarity
  • Easily decorated
  • Can be printed, hot stamped or metalized.
  • Gamma, Eto and E-beam sterilizable
  • Can be bonded to flexible PVC
  • Alcohol and lipid resistance
  • Resistance to most industrial and commercial cleaners
  • Resistance to most household cleaners
  • Resistant to most food additives
  • Residential dishwasher safe - top rack
  • Secondary operations include sonic welding, hotplate welding, ultrasonic bonding and adhesive bonding
  • Over-molding capability
Product Capabilities
  • Antistatic and indoor UV grades available
  • Available in natural and pre-colored
  • Color matching capabilities

Customer Productivity & Processing

  • 5 to 25% density advantage means more parts per pound of resin
  • Faster cycle time
  • Reduced energy and labor costs associated with processing
  • Lower processing temperatures by as much as 150F
  • No drying
  • Styrenic processing
  • Better thermal stability
  • More usable regrind and no black specs
  • Product consistency, color consistency
  • Easily colored at the press
  • Easy flow
  • Able to utilize existing tooling for PC, clear ABS, impact acrylic, PETG, polyesters, propionate (CAP), PVC and other polymers

Information provided by NOVA Chemicals.

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Water Absorption 0.10 %0.10 %24 hrs; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm0.0020 - 0.0060 in/inASTM D955
Melt Flow 5.6 g/10 min
@Load 5.00 kg,
Temperature 200 °C
5.6 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 6161ASTM D785
Tensile Strength, Yield 31.0 MPa4500 psi0.2 in/min; ASTM D638
Elongation at Break 53 %53 %0.2 in/min; ASTM D638
Modulus of Elasticity 2.34 GPa339 ksi0.2 in/min; ASTM D638
Flexural Strength 49.0 MPa7110 psi0.5 in/min; ASTM D790
Flexural Modulus 2.07 GPa300 ksi0.5 in/min; ASTM D790
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C190 °FAnnealed; ASTM D648
Vicat Softening Point 99.0 °C210 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.561.56ASTM D542
Haze 3.1 %3.1 %ASTM D1003
Transmission, Visible 87.5 %87.5 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 238 °C<= 460 °F
Rear Barrel Temperature 179 - 213 °C354 - 415 °F
Middle Barrel Temperature 185 - 218 °C365 - 424 °F
Front Barrel Temperature 191 - 224 °C376 - 435 °F
Melt Temperature 204 - 238 °C399 - 460 °F
Mold Temperature 27.0 - 54.0 °C80.6 - 129 °F
Drying Temperature 68.0 °C154 °F
Dry Time 2 hour2 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer
Asahi Kasei DELPET™ PM120N Acrylic (PMMA), Heat Resistant
Albis Plastics PC/Polyester 362/01 E UV Clear Unfilled
Ineos Nova Zylar® 220 Clear Impact Modified Acrylic Copolymer
Ineos Nova Zylar® 330 Clear Impact Modified Acrylic Copolymer

PNOVA172 / 55073

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.