MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ecovio® C2224 F Blend Biodegradable Polyester
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polylactic Acid (PLA) Biopolymer

Material Notes: Ecovio® F Blend C2224 is a biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic acid (PLA, NatureWorks®). Because of the PLA content Ecovio® F Blend C2224 consists of 45% of renewable resources. Ecoflex® F Blend is the coherent phase in the structure of Ecovio® F Blend C2224 transferring the beneficial film properties of Ecoflex® F Blend into the new film product.

Application: Ecovio® F Blend C2224 has been developed for the conversion to flexible films using a blown film process. Typical applications are packaging films, hygienic films, carrier bags and compost bags. In view of numerous factors influencing functionality and shelf life of Ecovio® films and finished articles made therof the production parameters have to be tested by the converters before utilization. Additionally sufficient field tests are required to ensure the right functionality of the articles made from Ecovio® F Blend C2224.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 - 1.26 g/cc0.0448 - 0.0455 lb/in³ISO 1183
Water Vapor Transmission 98.0 g/m²/day6.31 g/100 in²/dayASTM F1249
Oxygen Transmission Rate 860 cc/m²/day55.4 cc/100 in²/daydry; ASTM D3985
Melt Flow  <= 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
<= 2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 2.4 - 5.2 g/10 min
@Load 5.00 kg,
Temperature 190 °C
2.4 - 5.2 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5959ISO 868
Tensile Strength 27.0 - 35.0 MPa3920 - 5080 psiISO 527
Tensile Strength, Ultimate 27.0 - 35.0 MPa3920 - 5080 psiISO 527
Elongation at Break 250 - 320 %250 - 320 %ISO 527
Tensile Modulus 0.520 - 0.750 GPa75.4 - 109 ksiISO 527
Dart Drop Total Energy 380 J/cm0.712 ft-lb/milDIN 53373
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 - 120 °C230 - 248 °FDSC
 140 - 155 °C284 - 311 °FDSC
Vicat Softening Point 68.0 °C154 °FA/50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 85 %85 %ASTM D1003
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polylactic Acid (PLA) Biopolymer
BASF Ecovio® C2203 F Blend Biodegradable Polyester
BASF Ecovio® C2332 F Blend Biodegradable Polyester
FKuR Kunststoff Bio-Flex® F 7510 PLA Blend
Ex-Tech Plastics RenewTech™ BioPlastics Ingeo™ PLA

PBASG0008 / 131642

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.