MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Melinex® ST579 Polyester Film, 200 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® ST579 is a clear, heat stabilized polyester film that is primed on one surface for adhesion. Typical applications include flexible electronics, touch screens, displays, circuitry, and other industrial uses where high light transmission and excellent thermal stability are required.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 150 %150 %ASTM D882A
Film Elongation at Break, TD 100 %100 %ASTM D882A
Flexural Strength 137.9 MPa20000 psi
Coefficient of Friction 0.600.60
Coefficient of Friction, Static 0.400.40A-B; ASTM D1894
Film Tensile Strength at Break, MD 179 MPa26000 psiASTM D882A
Film Tensile Strength at Break, TD 200 MPa29000 psiASTM D882A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+8 - 1.00e+12 ohm-cm1.00e+8 - 1.00e+12 ohm-cm
Surface Resistivity per Square 1.00e+8 ohm1.00e+8 ohm
Dielectric Constant 2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
ASTM D150
Dielectric Strength 118 kV/mm3000 kV/in
 197 kV/mm5000 kV/inASTM D149
Dielectric Breakdown 10000 V10000 VASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 50.0 °C
10.0 µin/in-°F
@Temperature 68.0 - 122 °F
Melting Point 260 °C500 °F
Shrinkage, MD 1.0 %
@Temperature 150 °C,
Time 1800 sec
1.0 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.00 %
@Temperature 150 °C,
Time 1800 sec
0.00 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Haze 1.0 %1.0 %ASTM D1003
Gloss 140 %140 %
Transmission, Visible 90 %90 %TLT; ASTM D1003
 
Descriptive Properties
Coefficient of Hygroscopic Expansion0.000008 IN/IN/% RH40% - 80% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® ST580 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® ST730 Polyester Film
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge
DuPont Teijin Films Melinex® ST505 Polyester Film, 500 Gauge
DuPont Teijin Films Melinex® ST504 Polyester Film, 500 Gauge

PDTZ9249 / 139573

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.