MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Alcoa 7055-T77511 Aluminum Extrusions
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Alcoa introduced alloy 7055 in the -T7751 temper for plate and the -T77511 for extrusions in 1991. This alloy was developed for use in compression-dominated structures (such as upper wing structures, horizontal stabilizer, and keel beams) and provides advantages over alloy 7150 in compressive and tensile strengths while maintaining other important properties such as fracture toughness and corrosion resistance.

Information provided by Alcoa.

Key Words: Aluminium 7055-T77511; AA7055
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.86 g/cc0.103 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  634 MPa
@Thickness 25.4 mm
92000 psi
@Thickness 1.00 in
Longitudinal Direction
 641 MPa
@Thickness 25.4 mm
93000 psi
@Thickness 1.00 in
LT Direction
Tensile Strength, Yield  614 MPa
@Thickness 25.4 mm
89000 psi
@Thickness 1.00 in
Longitudinal Direction
 614 MPa
@Thickness 25.4 mm
89000 psi
@Thickness 1.00 in
LT Direction
Elongation at Break  10 %
@Thickness 25.4 mm
10 %
@Thickness 1.00 in
LT Direction
 11 %
@Thickness 25.4 mm
11 %
@Thickness 1.00 in
Longitudinal Direction
Compressive Yield Strength  621 MPa
@Thickness 25.4 mm
90000 psi
@Thickness 1.00 in
Longitudinal Direction
 648 MPa
@Thickness 25.4 mm
94000 psi
@Thickness 1.00 in
LT Direction
Fracture Toughness  26.4 MPa-m½
@Thickness 25.4 mm
24.0 ksi-in½
@Thickness 1.00 in
KIC, T-L
 28.6 MPa-m½
@Thickness 25.4 mm
26.0 ksi-in½
@Thickness 1.00 in
KIC, L-T
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 85.9 - 88.5 %85.9 - 88.5 %As remainder
Chromium, Cr <= 0.04 %<= 0.04 %
Copper, Cu 2.0 - 2.6 %2.0 - 2.6 %
Iron, Fe <= 0.15 %<= 0.15 %
Magnesium, Mg 1.8 - 2.3 %1.8 - 2.3 %
Manganese, Mn <= 0.05 %<= 0.05 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.10 %<= 0.10 %
Titanium, Ti <= 0.06 %<= 0.06 %
Zinc, Zn 7.6 - 8.4 %7.6 - 8.4 %
Zirconium, Zr 0.08 - 0.25 %0.08 - 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 7055-T7751 Plate
Kaiser 7068 T6, T6511 Rod & Bar
Aluminum 7055-T77511 Extrusions
Alcoa 7055-T7751 Aluminum Plate
Aluminum 7475-T7651

NALCOA98 / 176072

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.