MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Buckeye Polymers BP RPP 2008 T NAT Polypropylene, Talc Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resistance to some aggressive chemical agents. Buckeye Polymers can also customize these materials through the addition of UV packages, custom color matching, and processing additives.

    Product Features:
  • Increased stiffness and heat deflection
  • Good UV resistance
  • Industrial, appliance, construction markets
  • Good scratch and mar resistance
  • Appearance: Natural

    Forms: Pellets

    Processing Method: Injection Molding

    Information Provided by Buckeye Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 - 1.06 g/cc1.02 - 1.06 g/ccASTM D792
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm0.0080 - 0.012 in/inASTM D955
Melt Flow 6.0 - 10 g/10 min6.0 - 10 g/10 minASTM D1238
Ash 18 - 22 %18 - 22 %ASTM D5630
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 29.0 MPa>= 4200 psiASTM D638
Flexural Modulus >= 1.72 GPa>= 250 ksiASTM D790
Izod Impact, Notched >= 0.427 J/cm>= 0.800 ft-lb/inASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 199 X 134954 A Polypropylene (PP) Mineral - Flame Retardant - Non-PBB/PBDE - UV Resistant
Polykemi AB POLYfill PP CIP6015F VTUV Polypropylene, Mineral Reinforced, Heat and UV Stabilized
Phillips Sumika Marlex® CDB-300 Polypropylene Talc-Filled Impact Copolymer
Overview of materials for Polypropylene with 30% Talc Filler
Overview of materials for Acrylic, General Purpose, Molded

PBUCK029 / 104496

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.