MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chesterton ARC NVE SYSTEM Vinyl Ester Lining
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: Description: ARC NVE is a high performance, quartz reinforced, three-component, modified novolac vinyl ester lining capable of being applied to horizontal and vertical surfaces. The NVE system kit is comprised of a primer (NVE PC), top coat (NVE TC) and optional veil coat sealer (NVE VC) which is used in applications that require high impact and abrasion resistance combined with resistance to a wide range of solvents, acids, fats, oils, water and various chemicals at ambient as well as elevated temperatures.

Benefits:

  • Deep penetrating primer system allows for exceptionally high adhesion to prepared concrete
  • Integrated topcoat sealer system prevents migration or penetration of chemicals
  • High quartz loading ensure a compatible thermal coefficient of expansion providing long-term resistance to disbondment.
  • Graded quartz reinforcements allow for single lift vertical build application up to 3 meters (10 ft)
  • User friendly consistency makes installation and finishing fast and easy.

Applications: ARC NVE is generally used to repair and upgrade concrete surfaces or as a replacement for acid resistant tiles, phenolics, furans, conventional novalac epoxy, sulfonated concretes and other overlayments. It is formulated to be thermally compatible with concrete and its rapid curing allows areas to be returned to service in as little as 24 hours. ARC NVE is chosen over the ARC Concrete Composite Systems for its superior chemical resistance.

Suggested Uses:

  • Battery Rooms
  • Pickling & Plating Lines
  • Bleaching Areas
  • Sumps, Trenches & Pits
  • Chemical Containments
  • Pump & Equipment Bases
  • Chemical Loading Stations
  • Pickling Rooms
CAS: 100-42-5

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.24 g/cc0.0809 lb/in³Cured
Volatiles 2.2 %2.2 %EPA 24
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 9.915 MPa1438 psiASTM C307
Modulus of Elasticity 12.4 GPa1800 ksiFlexural
Flexural Strength 17.48 MPa2535 psiASTM C580
Compressive Strength 78.6 MPa11400 psiASTM C579
Adhesive Bond Strength >= 3.86 MPa>= 560 psiExcellent - 100% Concrete Failure
 
Thermal PropertiesMetricEnglishComments
CTE, linear 26.6 µm/m-°C14.8 µin/in-°FASTM C531
Maximum Service Temperature, Air 135 °C275 °FWet Continuous
 200 °C392 °FDry Continuous
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 26.0 °C
1.00 hour
@Temperature 78.8 °F
Foot Traffic
 60.0 min
@Temperature 26.0 °C
1.00 hour
@Temperature 78.8 °F
Light Load
 60.0 min
@Temperature 26.0 °C
1.00 hour
@Temperature 78.8 °F
Full Load
 90.0 min
@Temperature 21.0 °C
1.50 hour
@Temperature 69.8 °F
Foot Traffic
 90.0 min
@Temperature 21.0 °C
1.50 hour
@Temperature 69.8 °F
Light Load
 120 min
@Temperature 21.0 °C
2.00 hour
@Temperature 69.8 °F
Full Load
 150 min
@Temperature 16.0 °C
2.50 hour
@Temperature 60.8 °F
Foot Traffic
 180 min
@Temperature 16.0 °C
3.00 hour
@Temperature 60.8 °F
Light Load
 240 min
@Temperature 10.0 °C
4.00 hour
@Temperature 50.0 °F
Foot Traffic
 240 min
@Temperature 16.0 °C
4.00 hour
@Temperature 60.8 °F
Full Load
 360 min
@Temperature 10.0 °C
6.00 hour
@Temperature 50.0 °F
Light Load
 480 min
@Temperature 10.0 °C
8.00 hour
@Temperature 50.0 °F
Full Load
 960 min
@Temperature 26.0 °C
16.0 hour
@Temperature 78.8 °F
Full Chemical
 1440 min
@Temperature 21.0 °C
24.0 hour
@Temperature 69.8 °F
Full Chemical
 1680 min
@Temperature 16.0 °C
28.0 hour
@Temperature 60.8 °F
Full Chemical
 1920 min
@Temperature 10.0 °C
32.0 hour
@Temperature 50.0 °F
Full Chemical
 
Descriptive Properties
ColorGray
 Red
Thermal Compatibility to ConcretePassASTM C884

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Budd DSM-949, Diesel Grade SMC, Vinyl Ester, Black
Fibre Glast 1110 CC Vinyl Ester Resin (Casting Properties)
Devcon Brushable Ceramic - White Epoxy
Devcon Brushable Ceramic - Red, Blue Epoxy
Cookson Group Plaskon® 3100 Novolac Epoxy Molding Compound

PPTCHS015 / 138127

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.