MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubriplate SYN LUBE 22 PAO-Based Multi-Purpose Synthetic Fluid
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: PAO-based zinc free fluids formulated with state of the art additives to provide outstanding performance over extended drain intervals.

Applications: Syn-Lube 22, 32, 46, 68 & 100 are recommended for many types of rotary screw and piston type air compressors, hydraulic systems, blowers, and turbine oil applications.

Available in Pails and Drums

Information provided by Lubriplate

Key Words: Part Number L0968-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 2222ISO Grade
 138138Viscosity Index
Saybolt Viscosity at 100°F 129 SUS129 SUS
Saybolt Viscosity at 210°F 44 SUS44 SUS
Kinematic Viscosity at 40°C (104°F) 23 cSt23 cSt
Kinematic Viscosity at 100°C (212°F) 5.0 cSt5.0 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -56.7 °C-70.0 °F
Flammability Test 470470[°F] Fire Point
 >= 700>= 700[°F] Auto-Ignition
Flash Point 216 °C420 °F
 
Descriptive Properties
SAE No.5W

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubriplate SYN LUBE 32 PAO-Based Multi-Purpose Synthetic Fluid
Nye Lubricants 162 (SO) Synthetic Oil
Lubriplate SYN LUBE 68 PAO-Based Multi-Purpose Synthetic Fluid
Lubriplate SYN LUBE 46 PAO-Based Multi-Purpose Synthetic Fluid
Lubriplate SFGO Ultra-22 PAO-Based Synthetic Food Machinery Grade Fluid

WLUBR000 / 76046

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.