MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elkem (Bluestar Silicones) BLUESIL™ FLD 41V0.65 Fluid
Categories: Fluid

Material Notes: Description: BLUESIL FLD 41V0.65 is hexamethyl disiloxane.

Applications:

  • In the synthesis of silicone products as a production intermediate.
  • Volatile solvent.
  • Hydraulic fluid for low temperature use: Damping fluid; Lubricating release fluid; Heat transfer fluid.
Advantages:
  • Thick, non oily, volatile liquid.
  • ?Low surface tension.
  • Low freezing point.
  • Low variation in viscosity with temperature.
  • High compressibility.
  • Good dielectric properties.
  • Good resistance to oxidation.
  • Lack of ageing under the action of atmospheric agents.

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.760 g/cc0.760 g/cc
Viscosity 0.65 cP0.65 cPAverage
Kinematic Viscosity 0.58 - 0.72 cSt0.58 - 0.72 cSt
Vapor Pressure 0.0400 bar30.0 torr
Surface Tension 15.9 dynes/cm15.9 dynes/cm
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
Dielectric Constant 2.18
@Frequency <=100000 Hz
2.18
@Frequency <=100000 Hz
Dielectric Strength 14.0 kV/mm356 kV/in
Dissipation Factor 0.000010
@Frequency 100000 Hz
0.000010
@Frequency 100000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 1340 µm/m-°C
@Temperature 25.0 - 100 °C
744 µin/in-°F
@Temperature 77.0 - 212 °F
Specific Heat Capacity 2.90 J/g-°C0.693 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°F
Boiling Point 100 °C
@Pressure 0.1013 MPa
212 °F
@Pressure 14.69 psi
Pour Point -67.0 °C-88.6 °F
Flash Point -4.00 °C24.8 °Fclosed cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.373 - 1.3761.373 - 1.376
 1.3751.375Average
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Month
 
Descriptive Properties
Appearanceclear liquid free of foreign bodies
Color<40Hazen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 20 Polydimethylsiloxanic Fluids
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 100 Polydimethylsiloxanic Fluids
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 5 Polydimethylsiloxanic Fluids
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 50 Polydimethylsiloxanic Fluids
Elkem (Bluestar Silicones) BLUESIL™ FLD 48 V 100 Polydimethylsiloxane Fluid

PBLUST126 / 191109

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.