MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Lehvoss LUVOCOM® 1105/CF/30/EM PEEK with carbon fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Properties/attributes include: Very strong and stiff parts; low coefficient of thermal expansion. Dynamically-stressed parts moving at high velocity. Chemically- and hydrolytically- resistant parts, non flammable. Electrically conductive, suitable for continuous discharging of statically-generated electricity.

Automotive industry, textile machinery, medical- and precision engineering, aircraft industry. Typical uses include: Bearings, sleeves, control disks, gear wheels, pump impellers, gear parts.

Processing: During processing, the moisture content should not exceed 0.05%. To avoid internal stresses, a medium to high injection rate should be used. An increase in tool temperature may be helpful. Post-crystallization may lead to warpage at elevated operating temperatures. This can be counteracted by suitable heat treatment. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application. High-temperature polymers place increased demands on the tool steels employed.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/ccISO 1183
Moisture Absorption <= 0.100 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.100 %
@Temperature 73.4 °F,
Time 24.0 hour
Linear Mold Shrinkage 0.00050 - 0.0020 cm/cm0.00050 - 0.0020 in/inDIN 16901
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 245 MPa35500 psiISO 527-2
Elongation at Break 1.6 %1.6 %ISO 527-2
Modulus of Elasticity 27.0 GPa3920 ksiISO 527-2
Flexural Strength 370 MPa53700 psiISO 178
Flexural Modulus 23.0 GPa3340 ksiISO 178
Flexural Strain at Break 2.0 %2.0 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1fu
Charpy Impact, Notched  0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
ISO 179 eA
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 1e+05<= 1e+05IEC 60167
Surface Resistance <= 10000 ohm<= 10000 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C5.00 µin/in-°FDIN 53752
Thermal Conductivity 0.600 W/m-K4.16 BTU-in/hr-ft²-°FDIN 52612
Maximum Service Temperature, Air 250 °C482 °FContinuous; UL 746B
 280 °C536 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FISO 75-2/A
Vicat Softening Point 325 °C617 °FVST A; DIN ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 360 - 380 °C680 - 716 °F
Zone 1 360 - 370 °C680 - 698 °F
Zone 2 380 - 390 °C716 - 734 °F
Zone 3 390 - 400 °C734 - 752 °F
Melt Temperature 390 °C734 °F
Mold Temperature 170 - 190 °C338 - 374 °FSuggested Range
Drying Temperature  120 °C
@Time 21600 - 28800 sec
248 °F
@Time 6.00 - 8.00 hour
Dehumidifying dryer
 150 °C
@Time 10800 - 21600 sec
302 °F
@Time 3.00 - 6.00 hour
Dehumidifying dryer
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
Colornatural color (black)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lehvoss LUVOCOM® 1105/XCF/30 PEEK with carbon fiber
RTP Company RTP 2287 HF Polyetheretherketone (PEEK), Carbon Fiber - High Flow
RTP Company RTP 2281 HF Polyetheretherketone (PEEK), Carbon Fiber - High Flow
RTP Company RTP 2285 HF Polyetheretherketone (PEEK); Carbon Fiber - High Flow
Lehvoss LUVOCOM® EOG-400 PEEK with carbon fiber

PLUU8820 / 193779

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.