MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies

Search Results

The search phrase you entered, aisi 1020, is common to 20 materials, by searching on the exact phrase [ "aisi 1020" ] in the most common text fields.

Results are displayed up to a maximum of 200 materials per page. Follow the links below to view complete property information. If your material is not listed, please refer to our search help page for assistance in limiting your search.

Expand Search Results
By clicking on the "Broaden" button, MatWeb will continue to modify your search criteria in an effort to provide you with a better result set. Your search terms may be modified in the following ways: 1) We will search additional text fields    2) We will add conjunctions "AND" or "OR" between individual words (for multiple words)   3) We will search terms using wildcards (as if they are prefixes or suffixes) of individual words


Found 20 Results -- Page of 1 -- [Prev Page] [Next Page] --  view per page
Use Folder Contains  
Select Material Name
 1AISI 1020 Steel, cold rolled
 2AISI 1020 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
 3AISI 1020 Steel, hot rolled, quenched and tempered, 0.2% offset, 19-32 mm (0.75-1.25 in) round
 4AISI 1020 Steel, as rolled
 5AISI 1020 Steel, normalized at 870°C (1600°F)
 6AISI 1020 Steel, annealed at 870°C (1600°F)
 7AISI 1020 Steel, as rolled, 25 mm (1 in.) round
 8AISI 1020 Steel, annealed at 870°C (1600°F), furnace cooled 17°C (31°F) per hour to 700°C, air cooled, 25 mm (1 in.) round
 9AISI 1020 Steel, normalized at 925°C (1700°F), air cooled, 13 mm (0.5 in.) round
 10AISI 1020 Steel, normalized at 925°C (1700°F), air cooled, 25 mm (1 in.) round
 11AISI 1020 Steel, normalized at 925°C (1700°F), air cooled, 50 mm (2 in.) round
 12AISI 1020 Steel, normalized at 925°C (1700°F), air cooled, 100 mm (4 in.) round
 13AISI 1020 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 13 mm (0.5 in.) round
 14AISI 1020 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 25 mm (1 in.) round
 15AISI 1020 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 50 mm (2 in.) round
 16AISI 1020 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 100 mm (4 in.) round
 17JIS S20C Carbon Steel
 18JIS S20CK Carbon Steel
 19JIS SWRCH20A Carbon Steel
 20JIS SWRCH20K Carbon Steel
 
Found 20 Results -- Page of 1 -- [Prev Page] [Next Page] --  view per page


Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.