X-40 Cobalt Alloy (UNS R30031)
Most of the data in MatWeb has been supplied directly by companies in the supply chain -
the manufacturers, or, less commonly, distributors or fabricators. Other data
has been provided by standards organizations or from similar materials/known relationships by
the MatWeb staff. For more information about this specific material, see the following source(s):
Metals Handbook, Vol.1 - Properties and Selection: Irons, Steels, and High-Performance Alloys, ASM International 10th Ed. 1990.
Handbook of Superalloys - International Alloy Compositions and Designations Series M. J. Wahll, D. J. Maykuth, and H. J. Hucek, Battelle Press, Columbus, OH, (1979).