![USP Class VI Adhesives](/images/assets/MasterBondLogo.gif)
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.
Fire-refined Tough Pitch Copper with Silver, UNS C12900, H80 (15%) Temper shapes
Most of the data in MatWeb has been supplied directly by companies in the supply chain -
the manufacturers, or, less commonly, distributors or fabricators. Other data
has been provided by standards organizations or from similar materials/known relationships by
the MatWeb staff. For more information about this specific material, see the following source(s):
ASM Metals Reference Book, Third edition, Michael Bauccio, Ed. ASM International, Materials Park, OH, 1993.
ASM Specialty Handbook - Copper and Copper Alloys, edited by Joseph R. Davis, Davis & Associates, ASM International, Metals Park, OH, (2001).
Information provided by the Copper Development Association, Inc.