316 Stainless Steel, annealed bar
Most of the data in MatWeb has been supplied directly by companies in the supply chain -
the manufacturers, or, less commonly, distributors or fabricators. Other data
has been provided by standards organizations or from similar materials/known relationships by
the MatWeb staff. For more information about this specific material, see the following source(s):
Engineering Properties of Steels, Philip D. Harvey, editor, American Society for Metals, Metals Park, OH, (1982).
Handbook of Stainless Steels, Donald Peckner and I. M. Bernstein, McGraw-Hill Book Company, New York, NY, (1977)
Metals Handbook, Vol.1 - Properties and Selection: Irons, Steels, and High-Performance Alloys, ASM International 10th Ed. 1990.
Metals Handbook, Howard E. Boyer and Timothy L. Gall, Eds., American Society for Metals, Materials Park, OH, 1985.