Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Drill Down to All Materials Data Sheets
This series of pages is an inefficient set of links to all data sheets in MatWeb. We have several search tools, listed above, that give you more efficient methods to reach the information that you need.
Replacing...
Wellman Wellamid® GF33A099-HRN Glass Reinforced PA66
Wellman Wellamid® GF33A099-HRN Nylon 66, 33% Glass Reinforced, Hydrolysis Resistant
Wellman Wellamid® GF33AO99 HR 33% Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66
Wellman Wellamid® GF33AO99-HRBK 33% Glass Fiber Reinforced, Hydrolysis Resistant Nylon 66
Wellman Wellamid® GF43-66 XE-N 43% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Wellman Wellamid® GF43-66 XE-NBK1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66
Wellman Wellamid® GF43-66/6 XE-BK167A Nylon 66/6Glass, 43% Glass
Wellman Wellamid® GF43-66/6 XE-N 43% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Wellman Wellamid® GF43-66/6 XE-NBK1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6
Wellman Wellamid® GF60-66/6 XE-N 60% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Wellman Wellamid® GF60-66/6 XE-NBK1 60% Glass Fiber Reinforced, Engineering Grade Nylon 66/6
Wellman Wellamid® GFT13-66 XE-N 13% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Wellman Wellamid® GFT13-66 XE-NBK1 13% Glass Fiber Reinforced, Impact Modified Nylon 66
Wellman Wellamid® GFT13-66 XE-WT1 13% Glass Filled, Toughened Nylon 66
Wellman Wellamid® GFT1525-BK 15% Glass Fiber Reinforced, Impact Modified Nylon 6
Wellman Wellamid® GFT1525-BK Glass Fiber Reinforced, Impact Modified Nylon 6
Wellman Wellamid® GFT15N050-BK2 15% Glass Fiber Toughened Nylon 66
Wellman Wellamid® GFT15N050-N2 15% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Wellman Wellamid® GFT15N050-WBK 15% Glass Fiber Reinforced, Toughened, Weatherable Nylon 66
Wellman Wellamid® GFT1628-BK 17% Glass Fiber Reinforced, Impact Modified Nylon 66
Wellman Wellamid® GFT1675-N1 33% Glass Fiber Reinforced, Impact Modified Nylon 66
Wellman Wellamid® GFT1699-WBK1 13% Glass Fiber Reinforced, Weatherable Black Nylon 66
Wellman Wellamid® GFT1702-WBK1 33% Glass Fiber Reinforced, Impact Modified and Weatherable Nylon 66
Wellman Wellamid® GFT1835-WBK1 Nylon 66, 17% Glass Fiber Reinforced, Impact Modified
Wellman Wellamid® GFT33N051-N2 33% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Wellman Wellamid® GFT33N051-NBK2 Nylon 66, 33% Glass Fiber Reinforced, Impact Modified
Wellman Wellamid® GFT33NO51-NBK2 33% Glass Fiber Reinforced, Impact Modified Nylon 66
Wellman Wellamid® GFX1356-BK01 20% Glass Fiber Reinforced, Lubricated Nylon 6
Wellman Wellamid® GFX1356-BK01 Nylon 6, Glass Fiber Reinforced, Lubricated
Wellman Wellamid® GFX1624-BK(PTFE) 30% Glass Fiber Reinforced, Lubricated Nylon 66
Wellman Wellamid® GFX1717-BK1 Nylon 66, 43% Glass Fiber Reinforced, Silicone Lubricated
Wellman Wellamid® GFX1717-N1 43% Glass Fiber Reinforced, Silicone Lubricated Nylon 66
Wellman Wellamid® GFX1743-BK1(PTFE) 45% Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6
Wellman Wellamid® GFX1743-N1(PTFE) 45% Glass Fiber Reinforced, Enhanced Lubrication Nylon 66/6
Wellman Wellamid® GFX1872-N1 (PTFE) Nylon 66, 33% Glass Reinforced, Lubricated
Wellman Wellamid® GFX1872-N1(PTFE) Glass Fiber Reinforced, Lubricated Nylon PA66
Wellman Wellamid® GS1684-WBK1 25% Glass Sphere Filled Nylon 66
Wellman Wellamid® GS1791-N2 5% Glass Sphere Reinforced, Natural Nylon 66
Wellman Wellamid® GS1857-BK1 Nylon 66, 15% Glass Sphere Reinforced
Wellman Wellamid® GS1861-N1(PTFE) Nylon 66, 35% Glass Sphere Reinforced, Enhanced Lubrication
Wellman Wellamid® GS25/15-66 22L-N 25% Glass Sphere/15% Short Glass Fiber Reinforced Nylon 66, Lubricated
Wellman Wellamid® GS25-66 22LH-N 25% Glass Sphere Filled Nylon 66, Lubricated & Heat Stabilized
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated
Wellman Wellamid® GS25-66 22L-NBK1 Nylon 66, 25% Glass Sphere
Wellman Wellamid® GS40-60 42LH-N 40% Glass Sphere Filled Nylon 6, Lubricated & Heat Stabilized
Wellman Wellamid® GS40-60 42L-N 40% Glass Sphere Filled Nylon 6, Lubricated
Wellman Wellamid® GS40-60 42L-NBK1 40% Glass Sphere Reinforced Nylon 6
Wellman Wellamid® GS40-66 22L-Bk1 40% Glass Sphere Filled Nylon 66
Wellman Wellamid® GS40-66 22L-N 40% Glass Sphere Filled Nylon 66, Lubricated
Wellman Wellamid® GS40-66 22L-NBK1 Nylon 66, 40% Glass Sphere
Wellman Wellamid® GSF1849-N1 Nylon 66, 40% Glass Sphere/Fiber Reinforced
Wellman Wellamid® GSF25/15-66 22LH-N 40% Glass Sphere/Fiber Reinforced Nylon 66
Wellman Wellamid® GSF25/15-66 22L-N 40% Glass Sphere/Fiber Reinforced Nylon 66
Wellman Wellamid® GSF25/15-66 22L-NBK1 40% Glass Sphere/Fiber Reinforced Nylon 66
Wellman Wellamid® MR1873-EPBK1 Nylon 6, 40% Mineral
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized
Wellman Wellamid® MR340 42H-N 34% Mineral Reinforced Nylon 6, Heat Stabilized
Wellman Wellamid® MR340 42H-NBK1 Nylon 6, 34% Mineral Reinforced
Wellman Wellamid® MR409 22H-GY1 Nylon 66, 40% Mineral Reinforced
Wellman Wellamid® MR409 22H-N 40% Mineral Reinforced Nylon 66, Heat Stabilized
Wellman Wellamid® MR409 22H-NBK1 Nylon 66, 40% Mineral Reinforced
Wellman Wellamid® MR409 22H-NBK3 Nylon 66, 40% Mineral
Wellman Wellamid® MR409 22H-NBK4 40% Mineral Reinforced Nylon 66
Wellman Wellamid® MR410 22H-GY1 40% Mineral Reinforced Nylon 66
Wellman Wellamid® MR410 22H-N 40% Mineral Reinforced Nylon 66, Heat Stabilized
Wellman Wellamid® MR410 22H-NBK1 40% Mineral Reinforced Nylon 66
Wellman Wellamid® MR410 22H-WBK 40% Mineral Reinforced, Weatherable Black Nylon 66
Wellman Wellamid® MR410 42H-N 40% Mineral Reinforced Nylon 6, Heat Stabilized
Wellman Wellamid® MR410 42H-NBK1 40% Mineral Reinforced Nylon 6
Wellman Wellamid® MRB40K004-WT1 40% Mineral Reinforced Nylon 66
Wellman Wellamid® MRGF1475 BK01 20% Mineral/Glass Reinforced Nylon 66
Wellman Wellamid® MRGF1583-WT1 44% Mineral/Glass Reinforced Nylon 6
Wellman Wellamid® MRGF1647-BK1 Nylon 66, 40% Mineral/Glass Fiber Reinforced
Wellman Wellamid® MRGF1737-GY1 Nylon 6, 30% Mineral/Glass Reinforced
Wellman Wellamid® MRGF1882-BK1 Nylon 66, 40% Mineral/Glass Reinforced
Wellman Wellamid® MRGF25/15 22H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 66, Heat Stabilized
Wellman Wellamid® MRGF25/15 22H-NBK1 40% Mineral/Glass Reinforced Nylon 66
Wellman Wellamid® MRGF25/15 22H-NBK1/WE-1364 40% Mineral/Glass Reinforced Nylon 66
Wellman Wellamid® MRGF25/15 42H-BK167A Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced
Wellman Wellamid® MRGF25/15 42H-BK848 (Interior) 40% Mineral/Glass Fiber Reinforced, 848 Black Color Match Nylon 6
Wellman Wellamid® MRGF25/15 42H-BKDX9 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced
Wellman Wellamid® MRGF25/15 42H-BKJA6A Nylon 6, 25% Mineral and 15% Glass Reinforced
Wellman Wellamid® MRGF25/15 42H-GY1 40% Mineral/Glass Fiber Reinforced Nylon 6
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Wellman Wellamid® MRGF25/15 42H-N1/WE1705-N1 40% Mineral/Glass Fiber Reinforced Nylon 6
Wellman Wellamid® MRGF25/15 42H-N2/WE1705-N2 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced
Wellman Wellamid® MRGF25/15 42H-NBK1 40% Mineral/Glass Fiber Reinforced Nylon 6
Wellman Wellamid® MRGF25/15 42H-WBK Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced, Weatherable Grade
Wellman Wellamid® MRGF25/25 22H-GY1 Nylon 66, 25% Mineral and 25% Glass Reinforced
Wellman Wellamid® MRGF25/25 22H-NBK1 Nylon 66, 25% Mineral and 25% Glass Reinforced
Wellman Wellamid® MRGF30/10 42H-GY1 Nylon 6, 30% Mineral and 10% Glass Reinforced
Wellman Wellamid® MRGF30/10 42H-GY2 Nylon 6, 40% Glass/Mineral
Wellman Wellamid® MRGF30/10 42H-N 30% Mineral/10% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Wellman Wellamid® MRGF30/10 42H-N Mineral / Glass Reinforced Nylon 6
Wellman Wellamid® MRGF30/10 42H-NBK1 Nylon 6, 30% Mineral and 10% Glass Reinforced
Wellman Wellamid® MRGF3820-N 38% Mineral/Glass Reinforced Nylon 66
Wellman Wellamid® MRGF3822-BK 38% Mineral/10% Glass Fiber Reinforced Nylon 66, Heat Stabilized
Wellman Wellamid® MRGFX1393-N 40% Mineral/Glass Reinforced, Silicone Lubricated Nylon 6
Wellman Wellamid® MRGFX1393-N Mineral / Glass Reinforced Nylon 66
Wellman Wellamid® MRGFX1716-BK1 40% Mineral/Glass Reinforced, Silicone Lubricated Nylon 6
Wellman Wellamid® MRGST1715-WBK1 Nylon 6, 25% Mineral and Glass Sphere Reinforced, Impact Modified, Weatherable Grade
Wellman Wellamid® MRT1487 BK 32% Mineral Reinforced, Toughened Grade Nylon 66
Wellman Wellamid® MRT1487 BK Nylon 66, 32% Mineral Reinforced
Wellman Wellamid® MRT1487 N Nylon 66, 32% Mineral Reinforced, Impact Modified
Wellman Wellamid® MRT1487-N Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized
Wellman Wellamid® NB1803E-BK Nylon/Polypropylene Alloy
Wellman Wellamid® NY1599-BK Unfilled Nylon 66
Wellman Wellamid® NY1599-BK11 Unfilled Nylon 66
Wellman Wellamid® NY1599-GY Unfilled Nylon 66
Wellman Wellamid® NY1599-N Unfilled Nylon 66
Wellman Wellamid® NY1615-BK Unfilled Nylon 66
Wellman Wellamid® NY1718-N1 General Purpose Nylon 6
Wellman Wellamid® NY1733-GY1 Lubricated, Nucleated, Unfilled Nylon 6
Wellman Wellamid® NY1820-BK1(PTFE) Lubricated, Heat Stabilized Nylon 66
Wellman Wellamid® NY1875-BK1 Nylon 66, Unfilled
Wellman Wellamid® NY-4000 Nylon 6, Engineering Grade
Wellman Wellamid® T423-BK10 Mineral Reinforced Nylon 6, Heat Stabilized
Wellman Wellamid® T512-BK 15% Talc/Glass Reinforced, Dimensionally Stable Grade Nylon 6
Wellman Wellamid® T-731E-BK 10% Reinforced Abrasion Resistant Nylon 6
Wellman Wellamid® WE1359 25% Glass Sphere Filled, Toughened Nylon 66
Wellman Wellamid® WE1408 13% Glass Fiber Reinforced Engineering Grade Nylon 66
Wellman Wellamid® WE1410 43% Glass Fiber Reinforced Nylon 66
Wellman Wellamid® XT1482-BK High Impact Nylon 66
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Wellman Wellamid® XT1482-WT1 High Impact Nylon 66
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66
Wellman Wellamid® XT1486-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Wellman Wellamid® XT1573-N Impact Modified Nylon 66
Wellman Wellamid® XT1606-N Impact Modified Nylon 66
Wellman Wellamid® XT1627-BK2 High Impact Nylon 66
Wellman Wellamid® XT1627-GY1 High Impact Nylon 66
Wellman Wellamid® XT1627-WBK2 High Impact, Weatherable Nylon 66
Wellman Wellamid® XT1668-BK1 High Impact Nylon 66
Wellman Wellamid® XT1816-BK1 Toughened Nylon 66
Wellman Wellamid® XT1863-BK1 Impact Modified Nylon 66
Wellman Wellamid® XT1867-BK1 High Impact Nylon 66
Wellman Wellpet® FRGF116-BK1 Polyethylene Terephthalate, 30% Glass Fiber Reinforced, Flame Retardant
Wellman Wellpet® GF100-BK1 PET, 30% Glass Fiber Reinforced
Wellman Wellpet® GF100-N1 30% Glass Fiber Reinforced, Natural PET
Wellman Wellpet® MRGF101-GY1 PET, 29% Mineral/Glass Fiber Reinforced
Wellman Wellpet® MRGF102-BK1 PET, 35% Mineral/Glass Fiber Reinforced
Wellman Wellpet® PR109-N1 Unfilled PET
Wellman Wellpet® PR118-N2 Unfilled Polyester PET
Werkstoff 1.4911LN, FE-NM38 Superalloy
Werkstoff 1.4914LN, Fe-PM36, RNOD Superalloy
Wessex Emisshield™ M Series Nanoparticle Ceramic Coating
Wessex Emisshield™ ST Series Nanoparticle Ceramic Coating
Wessex Emisshield™ STG Series Nanoparticle Ceramic Coating
Western Red Cedar Plywood Sheathing
Western White Pine
Westlake 1185 PVC
Westlake 1195 PVC
Westlake 1195B Low molecular weight PVC resin
Westlake 1230P PVC
Westlake 1230S PVC
Westlake 2055 Low molecular weight, general purpose, PVC suspension resin
Westlake 2060 Low molecular weight, film and medical grade, PVC suspension resin
Westlake 2070 Low molecular weight, film and medical grade, PVC suspension resin.
Westlake 2079 Low molecular weight, film and medical grade, PVC suspension resin
Westlake 2082 Medium-low molecular weight, film and medical grade, PVC suspension resin
Westlake 2100 Medium-high molecular weight, film and medical grade, PVC suspension resin
Westlake 2110 High molecular weight, film and medical grade, PVC suspension resin
Westlake 2110M High molecular weight, medical grade, PVC suspension resin
Westlake 5265 Low molecular weight PVC suspension resin
Westlake 5305 Low molecular weight PVC suspension resin
Westlake 5385 Medium molecular weight PVC suspension resin
Westlake 5415 High molecular weight PVC suspension resin
Westlake DA502AA 12% EVA Copolymer (Experimental Product)
Westlake DA591 9.0% Ethylene Vinyl Acetate Copolymer
Westlake EB169 Low Density Polyethylene
Westlake EB171 MDPE Medium Density Polyethylene
Westlake EB403 Low Density Polyethylene
Westlake EB412 Low Density Polyethylene
Westlake EB502 12.5% EVA Copolymer
Westlake EB561 6.5% Ethylene Vinyl Acetate Copolymer
Westlake EBAC® Plus SP1903 18% Ethylene Butyl Acrylate Copolymer
Westlake EBAC® SP1802 22.5% Ethylene Butyl Acrylate Copolymer
Westlake EBAC® SP1806 17.5%, Ethylene-Methyl Acrylate Copolymer
Westlake EBAC® SP2810 16% EBA copolymer
Westlake EC 475 Low Density Polyethylene
Westlake EC 480 Low Density Polyethylene
Westlake EC1390AA Low Density Polyethylene
Westlake EC1550AA Low Density Polyethylene
Westlake EC1924AA Low Density Polyethylene
Westlake EC4041AA Low Density Polyethylene
Westlake EC4042AA Low Density Polyethylene
Westlake EC4056AA Low Density Polyethylene
Westlake EC471 Low Density Polyethylene
Westlake EC472 Low Density Polyethylene
Westlake EC474AA Low Density Polyethylene
Westlake EC476AA Low Density Polyethylene
Westlake EC477AA Low Density Polyethylene
Westlake EC478AA Low Density Polyethylene
Westlake EC479AA Low Density Polyethylene
Westlake EC482 Low Density Polyethylene
Westlake EC483 Low Density Polyethylene
Westlake EC800AA Low Density Polyethylene
Westlake EC808AA Low Density Polyethylene
Westlake EC811AA Low Density Polyethylene
Westlake EC812AA Low Density Polyethylene
Westlake EC850AA Low Density Polyethylene
Westlake EF 303 Low Density Polyethylene
Westlake EF 316 Low Density Polyethylene
Westlake EF 320 Low Density Polyethylene
Westlake EF 442 Low Density Polyethylene
Westlake EF 466 Low Density Polyethylene
Westlake EF 607 Low Density Polyethylene
Westlake EF 636 Low Density Polyethylene
Westlake EF1803 Low Density Polyethylene
Westlake EF1807 Low Density Polyethylene
Westlake EF1813 Low Density Polyethylene
Westlake EF1820 Low Density Polyethylene
Westlake EF1925 Low Density Polyethylene
Westlake EF310 Low Density Polyethylene
Westlake EF311 Low Density Polyethylene
Westlake EF313 Low Density Polyethylene
Westlake EF378 Low Density Polyethylene
Westlake EF403 Low Density Polyethylene
Westlake EF4060 Low Density Polyethylene
Westlake EF412 Low Density Polyethylene
Westlake EF413 Low Density Polyethylene
Westlake EF418 Low Density Polyethylene
Westlake EF421 Low Density Polyethylene
Westlake EF422 Low Density Polyethylene
Westlake EF424 Low Density Polyethylene
Westlake EF443 Low Density Polyethylene
Westlake EF444 4.7% Ethylene Vinyl Acetate Copolymer
Westlake EF464 Low Density Polyethylene
Westlake EF522 12% Ethylene Vinyl Acetate Copolymer
Westlake EF524 14.5% Ethylene Vinyl Acetate Copolymer
Westlake EF528 18.5% Ethylene Vinyl Acetate Copolymer
Westlake EF532 12% EVA Copolymer (Experimental Product)
Westlake EF600 Low Density Polyethylene
Westlake EF601 Low Density Polyethylene
Westlake EF602 Low Density Polyethylene
Westlake EF603 Low Density Polyethylene
Westlake EF606 Low Density Polyethylene
Westlake EF608 Low Density Polyethylene
Westlake EF612 Low Density Polyethylene
Westlake EF677 Low Density Polyethylene
Westlake EF706 Low Density Polyethylene
Westlake EF796 Low Density Polyethylene
Westlake EF808 Low Density Polyethylene
Westlake EF902 Low Density Polyethylene
Westlake EF923 Low Density Polyethylene
Westlake EF975 Low Density Polyethylene
Westlake EG378 Low Density Polyethylene
Westlake EG412 Low Density Polyethylene
Westlake EG417 Low Density Polyethylene
Westlake ELEVATE® DA539 Ethylene Vinyl Acetate Copolymer
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.