MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman tetra-DUR N 4303 Bulk Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: Mechanical high grade standard product.

Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stability, color retention, chemical stability, zero shrink/class-A-surface, and uniform color.

Information provided by Bulk Molding Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 - 2.00 g/cc0.0650 - 0.0723 lb/in³ISO 1138
Linear Mold Shrinkage 0.00 - 0.0010 cm/cm0.00 - 0.0010 in/inprocessing; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 35.0 - 45.0 MPa5080 - 6530 psiISO 527
Flexural Strength 100 - 140 MPa14500 - 20300 psiISO 178
Flexural Modulus 10.0 - 14.0 GPa1450 - 2030 ksiISO 178
Compressive Strength 150 - 170 MPa21800 - 24700 psiISO 604
Charpy Impact Unnotched 3.00 - 4.00 J/cm²14.3 - 19.0 ft-lb/in²ISO 179
Charpy Impact, Notched 3.00 - 4.00 J/cm²14.3 - 19.0 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 4.5
@Frequency 100 Hz
4.5
@Frequency 100 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm
@Thickness 1.00 mm
635 kV/in
@Thickness 0.0394 in
IEC 60243
Dielectric Loss Index <= 0.030
@Frequency 100 Hz
<= 0.030
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 - 25.0 µm/m-°C10.0 - 13.9 µin/in-°FVDE 0304T1
Deflection Temperature at 1.8 MPa (264 psi) >= 240 °C>= 464 °FISO 75
Flammability, UL94 HBHB
Shrinkage 0.00 - 0.050 %0.00 - 0.050 %post molding; ISO 2577
 
Descriptive Properties
Water Absorption>40 mg/1dISO 62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman tetra-DUR L 4305 Bulk Molding Compound
A. Schulman tetra-DUR F 4401 Bulk Molding Compound
A. Schulman tetra-DUR F 4308 Bulk Molding Compound
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP
A. Schulman tetra-DUR N 4203 Bulk Molding Compound

PBMC905 / 123369

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.