MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Nioro™ Mac-Nioro™-WM Braze Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy; Solder/Braze Alloy

Material Notes: High-purity gold/copper/nickel alloy for vacuum brazing.

Applications:

  • Aero-engines (OEM and repair)
  • Aerospace fuel-line assemblies
  • Vacuum tubes
  • Wave guide and Klystron assemblies
  • Power supply surge arrestors
  • Automotive components

information provided by Morgan Advanced Materials

Key Words: Braze Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 15.7 g/cc0.567 lb/in³
Vapor Pressure 1.32 bar
@Temperature 800 °C
988 torr
@Temperature 1470 °F
calculated
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 792 MPa115000 psi
Elongation at Break 12 - 15 %12 - 15 %2 in/50mm gage section
Compressive Yield Strength 686 MPa99500 psi0.2% offset
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000275 ohm-cm0.0000275 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.5 µm/m-°C
@Temperature 20.0 - 850 °C
9.72 µin/in-°F
@Temperature 68.0 - 1560 °F
Thermal Conductivity 28.0 W/m-K194 BTU-in/hr-ft²-°Fcalculated
Melting Point 950 - 950 °C1740 - 1740 °F
Solidus 950 °C1740 °F
Liquidus 950 °C1740 °F
 
Component Elements PropertiesMetricEnglishComments
Cadmium, Cd <= 0.0010 %<= 0.0010 %
Gold, Au 82 %82 %nominal
Lead, Pb <= 0.0020 %<= 0.0020 %
Nickel, Ni 18 %18 %nominal
Zinc, Zn <= 0.0010 %<= 0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Nioro™ ABA Mac-Nioro™ABA-WM Braze Alloy
Morgan Advanced Ceramics Paniro™ Mac-Palniro™7-WM Braze Alloy
Morgan Advanced Ceramics Nicoro™ Mac-Nicoro™-WM Braze Alloy
Morgan Advanced Ceramics 50Au-50Cu Mac-560Au/50 Cu-WM Braze Alloy
Morgan Advanced Ceramics Mac-35 Au/65 Cu-WM Braze Alloy

CMORF8002 / 203479

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.