MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® X7293 black 9.7507 Nylon 12, Extrusion/Tubing Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Extrusion/Tubing Grade

Material Notes: High viscosity, plasticized, impact modified, heat- and light-stabilized polyamide 12 compound. VESTAMID® X7293 is a plasticized polyamide 12 compound with heat and light stabilizer for the extrusion of flexible tubing and hose, especially for automotive applications according to DIN 73378, (PA 12-HIPHL, Type 1), ISO/DIS 7628-1 (PA 12-HIPEHL, Type 1) and SAE J844. VESTAMID® X7293 is distinguished by an easy processing as well as by a high impact strength at low temperatures. Properties of compounds based on Polyamide 12 vary little with changing humidity due to low moisture absorption. Parts made of this semicrystalline material are characterized by exceptional impact strength, low coefficient of friction and good chemical resistance. VESTAMID® X7293 is supplied as cylindrical granules, ready for use, in moisture-proof bags.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Moisture Absorption 0.500 %0.500 %Sim. to ISO 62
Melt Flow 52.9 g/10 min
@Load 5.00 kg,
Temperature 275 °C
52.9 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 42.0 MPa6090 psiISO 527
Tensile Strength, Yield 27.0 MPa3920 psiISO 527
Elongation at Break >= 50 %>= 50 %Nominal; ISO 527
 265 %265 %ISO 527
Elongation at Yield 32 %32 %ISO 527
Tensile Modulus 0.410 GPa59.5 ksiISO 527
50% Modulus 26.0 MPa
@Strain 50 %
26.0 MPa
@Strain 50 %
ISO 527
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Complete Break; ISO 179/1eA
 12.0 J/cm²
@Temperature 23.0 °C
57.1 ft-lb/in²
@Temperature 73.4 °F
Partial Break; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 62631-3-1
Dielectric Constant  4.6
@Frequency 1e+6 Hz
4.6
@Frequency 1e+6 Hz
IEC 60243-1
 11
@Frequency 100 Hz
11
@Frequency 100 Hz
IEC 60243-1
Dielectric Strength 30.0 kV/mm762 kV/inAC, S20/P50; Sim. to IEC 60243-1
Dissipation Factor  0.19
@Frequency 1e+6 Hz
0.19
@Frequency 1e+6 Hz
IEC 62631-2-1
 0.20
@Frequency 100 Hz
0.20
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 575 V575 Vtest solution A, 100 drops value; IEC 60112
 600 V600 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 180 µm/m-°C
@Temperature 23.0 - 55.0 °C
100 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°C
@Temperature 23.0 - 55.0 °C
100 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point 172 °C342 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C113 °FISO 75-1/-2
Vicat Softening Point 130 °C266 °FMethod B: 10 N, 50 K/h; ISO 306
 165 °C329 °FMethod A: 10 N, 50 K/h; ISO 306
Glass Transition Temp, Tg 13.0 °C55.4 °FISO 11357-1/-2
Flammability Test  1.0
@Thickness 1.60 mm
1.0
@Thickness 0.0630 in
IEC 60695-11-10
 1.0
@Thickness 3.20 mm
1.0
@Thickness 0.126 in
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK873 / 243080

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.