MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bada BADADUR® PBT8 GF30 natural PBT, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Medium viscosity, 30% glass fiber reinforced PBT injection molding grade with very good mechanical properties

Information provided by Bada

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³ISO 1183
Moisture Absorption 0.130 %0.130 %50% r.h.; ISO 62
Water Absorption at Saturation 0.37 %0.37 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 140 MPa20300 psi5 mm/min; ISO 527-1/2
Elongation at Break 2.6 %2.6 %5 mm/min; ISO 527-1/2
Tensile Modulus 10.0 GPa1450 ksi1 mm/min; ISO 527-1/2
Flexural Strength 210 MPa30500 psiISO 178
Izod Impact, Notched (ISO)  9.00 kJ/m²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  5.50 J/cm²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC-62631-3-1
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC-62631-3-2
Dielectric Constant 4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
IEC-62631-2-1
Dielectric Strength 29.0 kV/mm737 kV/inIEC-60243-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC-62631-2-1
Comparative Tracking Index 450 V450 VIEC-60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C19.4 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 95.0 µm/m-°C52.8 µin/in-°FISO 11359-2
Melting Point 223 °C433 °F10 K/min; ISO 3146
Maximum Service Temperature, Air 170 °C338 °Fsome hours; EC-60216
 140 °C
@Time 7.20e+7 sec
284 °F
@Time 20000 hour
EC-60216
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75-1/2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75-1/2
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 275 °C482 - 527 °F
Mold Temperature 60.0 - 100 °C140 - 212 °F
Drying Temperature <= 120 °C<= 248 °F
Dry Time 4.00 hour4.00 hour
Moisture Content <= 0.040 %<= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBADA355 / 287188

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.