MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions HTX Ultra LA426P PVC Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, High Impact

Material Notes: Geon HTX Ultra LA426 modified for improved paint adhesion, better stability and metal release. Developed as a substrate material.

Recommend drying material for a minimum of 2 hours at 160 degrees Fahrenheit. Physical properties based on Geon HTX Ultra LA426P natural 0000.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 77
@Time 15.0 sec
77
@Time 0.00417 hour
ASTM D2240
Tensile Strength, Yield 37.9 MPa5500 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.03 GPa294 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 67.7 MPa9820 psiASTM D790
Flexural Modulus 2.05 GPa297 ksiASTM D790
Izod Impact, Notched 6.25 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
11.7 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
Dart Drop Total Energy  44.5 J/cm
@Temperature 23.0 °C
0.0834 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125 Dart; ASTM D4226
 70.7 J/cm
@Temperature 23.0 °C
0.132 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125 Dart; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 83.0 µm/m-°C46.1 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi)  93.9 °C
@Thickness 3.18 mm
201 °F
@Thickness 0.125 in
Annealed; ASTM D648
 93.9 °C
@Thickness 3.18 mm
201 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  86.1 °C
@Thickness 3.18 mm
187 °F
@Thickness 0.125 in
Unannealed; ASTM D648
 87.8 °C
@Thickness 3.18 mm
190 °F
@Thickness 0.125 in
Annealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 379 °F
 
Descriptive Properties
Ease of SizingAcceptable
FeaturesGood Adhesion
 High Impact Resistance
 High Stiffness
FormsPellets
Generic NamePolyvinyl Chloride Alloy
Processing MethodExtrusion
PVC Cell Classification15225ASTM D1784
 4-41211-64-0000ASTM D4216
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesProfiles

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PH1PN8215 / 102051

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.