MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) PURELL PE 1840 H 950 LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Base Polymer: Polyethylene Low Density

Color: White

Market Segment: Medical/Personal Care

Application Area: Packaging

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ISO 1183
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 45
@Time 15.0 sec
45
@Time 0.00417 hour
ISO 868
Tensile Strength 11.0 MPa1600 psiISO 527
Tensile Modulus 0.145 GPa21.0 ksiISO 527
Flexural Strength 7.00 MPa1020 psiISO 178
Flexural Modulus 0.145 GPa21.0 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 90.0 °C194 °FA50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 °C356 °FInjection molding
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °FInjection molding
 
Descriptive Properties
Base PolymerPolyethylene Low Density
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accucomp Polyethylene LD0102L Low Density
A. Schulman CP775-01 Molding Grade, Low Density Polyethylene
Mocom (ALBIS) PURELL PE 1810 E 99950 LDPE
Mocom (ALBIS) PURELL PE 1810 E 93410 LDPE
Celanese 7205 LDPE polymer for flexible packaging and tubing

PALBIS8342 / 242401

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.