SCG™ PVC PG740 is a high molecular weight homopolymer paste PVC resin, produced by TPC Paste Resin Co., Ltd. under OxyChem’s HYBRID technology. Applications: Top layer for synthetic leather, tarpaulin, fabric coating products, PVC flooring products, strand coating products, mesh coating products, conveyor belts, industrial glove, auto sealants, mastic, logo, toys, handles and grips of hand tools, printing ink. Features: Low viscosity and good viscosity stability. Good foam quality. Excellent air release. High physical strength. Good heat stability. Information provided by SCG. |