MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin ZEFFLE GK-570 Tetrafluoroethylene and Vinyl Monomer
Categories: Gas

Material Notes: A solvent based paint resin with excellent weather, chemical, and stain resistance. GK-570 is a standard grade of all GK series.

Introduction: ZEFFLE GK-570 is a copolymer of tetrafluoroethylene and vinyl monomer. It does not include chlorine which may cause yellowing; Excellent weather resistance, corrosion protection, chemical resistance, and dirt removability; Gloss and color can be controlled easily; Variety of substrate can be chosen due to lower curing temperature. Even ambient temperature can be taken by selecting curing agent; Good compatibility with wide range of isocyanate curing agent. Melamine can also be used; Can be formulated for paint by spray, brush, roller, etc.; Can be used for versatile purposes

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 65.0 %65.0 %Dried by 150? for 1 hour
 
Chemical PropertiesMetricEnglishComments
Acid Value 3.00 - 4.003.00 - 4.00[mg KOH/g]
 
Descriptive Properties
AppearanceLight yellow clear liquid
Hydroxyl value63 mg KOH/g
Solvent>97%n-Butyl acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDAIK9684 / 327124

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.