MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALCOM® PP 620/2 GY1073-10MCF PP
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Base Polymer: Polypropylene Homopolymer

Color: grey, metallic

Special Features: Flow line optimized, low tendency to flow lines, slip agent, high flow

Application Area: Domestic appliances

Typical Application: Housings

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0060 - 0.020 cm/cm
@Time 86400 sec
0.0060 - 0.020 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.020 cm/cm
@Time 86400 sec
0.0060 - 0.020 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 70 g/10 min
@Load 2.16 kg,
Temperature 230 °C
70 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 30.0 MPa4350 psiISO 527
Elongation at Break 10 %10 %ISO 527
Tensile Modulus 1.80 GPa261 ksiISO 527
Flexural Strength 44.0 MPa6380 psiISO 178
Flexural Modulus 1.60 GPa232 ksiISO 178
Charpy Impact Unnotched 3.50 J/cm²16.7 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 95.0 °C203 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 270 °C392 - 518 °FInjection molding
Mold Temperature 20.0 - 70.0 °C68.0 - 158 °FInjection molding
 
Descriptive Properties
Base PolymerPolypropylene Homopolymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALBIS8574 / 242633

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.