MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALCOLOR® Function POM LE A BK1226-07 Color additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: For use in: Polyoxymethylene Copolymer

Filler/Additive System: Low emission

Special Features: Free from cadmium, lead and diarylide pigments, low emission, high flow, dust-free, high dispersibility, high additive content

Market Segment: Various

Application Area: Injection molded parts, extruded parts, blow molded parts

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 280 °C<= 536 °FThermal Stability Colorant
Drying Temperature  100 - 110 °C
@Time 7200 - 10800 sec
212 - 230 °F
@Time 2.00 - 3.00 hour
in a dry air (desiccant) dryer
 100 - 110 °C
@Time 10800 - 18000 sec
212 - 230 °F
@Time 3.00 - 5.00 hour
in air circulating dryer
 
Descriptive Properties
Base PolymerPolyoxymethylene Copolymer
ColorBlack
Dosage2-4%injection molding
Light Fastness Colorantblue woolscale 8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mocom (ALBIS) ALCOM® POM 770/1 MO2 POM, 2% MoS2 Reinforced
Asahi Kasei TENAC™ 2010 Homopolymer Acetal (POM), High viscosity
Mocom (ALBIS) ALCOM® POM 770/1 SI2 POM, 2% Silicone
Mocom (ALBIS) ALCOM® POM 770/1 PTFE18 SI2 POM, 20% PTFE/Silicone
Mocom (ALBIS) ALCOM® POM 770/1 GF20 PTFE15 POM, 20/15% Glass/PTFE Reinforced

PALBIS8015 / 242074

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.