MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ChevronTexaco Polystar® CVJ
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Base oil
  4. Unknown amount of work.

CPS Number: 222013; MSDS Number: 8659

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 9696Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 620 SUS620 SUSSee Note 3.
Saybolt Viscosity at 210°F 69.5 SUS69.5 SUSSee Note 3.
Kinematic Viscosity at 40°C (104°F) 118 cSt118 cStSee Note 3.
Kinematic Viscosity at 100°C (212°F) 12.5 cSt12.5 cStSee Note 3.
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Load Wear Index 5757
Four Ball Wear 0.600 mm0.0236 inScar Diameter
Penetration 160160Cold test, 6h, See Note 4
Penetration P(60), 1/10 mm 312312Unknown Amount of Work, 25°C (77°F)
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °FSee Note 2.
Minimum Service Temperature, Air -40.0 °C-40.0 °FSee Note 1.
Dropping Point 243 °C469 °F
 
Descriptive Properties
Bearing Rust ProtectionPass
ColorCream
TextureSmooth
Thickener, %11.5Polyurea

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco NLGI 2 SRI Grease OEM
ChevronTexaco NLGI 2 SRI Grease
ChevronTexaco Rykon® 1426 Premium Grease
ChevronTexaco Polystar® Synthetic 4602 NLGI Grade
ChevronTexaco Polystar® RB NLGI Grade 2

WTEXA263 / 77142

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.