MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

KaMin Kamintex® D Kaolin Clay - Calcined, high solids
Categories: Ceramic; Clay; Kaolin Clay

Material Notes: Kamintex® D is a high brightness, calcined clay designed for use in coating applications requiring high solids applications.

Industry: PAPER & PACKAGING

Uses: Coated 1S Label, Coated Bleached Board, Coated Recycled Board, Coated Natural Kraft, Lightweight Coated Paper, Coated Groundwood, Thermal Paper, Uncoated Freesheet, Uncoated Groundwood

Information provided by KaMin LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 58.5 - 59.5 %58.5 - 59.5 %Slurry
Brightness 92 - 93 %92 - 93 %Reflectance (TAPPI)
Particle Mesh Size 325 Mesh325 Mesh0.005% Retained
pH 6 - 86 - 8100 g/250 ml H2O Slurry
 
Descriptive Properties
CAS Number1332-58-7
Physical FormSlurry
Shipping PointSandersville, GA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kaolinite (Al2O3-2SiO2-2H2O)
KaMin Polygloss® 90 Kaolin Clay - Ultrafine, high brightness
KaMin Polyfil® WC-426 Kaolin Clay - Calcined
KaMin Polyfil® 70 Kaolin Clay - Calcined
KaMin Lithosperse® 7005CS Kaolin Clay - Surface Treated

CKAMAN911 / 178382

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.