MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asahi Kasei Lynex-T TFC64N Acetal Copolymer, Conductive Grade
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Acetal copolymer-based alloy with excellent electrical conductivity.

Applications: Electroconductive parts.

Key Words: POM; Polyoxymethylene, Polyacetal
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ASTM D792
Water Absorption 0.20 %0.20 %ASTM D570
Linear Mold Shrinkage 0.013 - 0.016 cm/cm0.013 - 0.016 in/inAsahi Chemical test
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ASTM D785
Hardness, Rockwell R 110110ASTM D785
Tensile Strength, Ultimate 37.3 MPa5410 psi5 mm/min; parallel to flow; ASTM D638
Elongation at Break 3.0 %3.0 %5 mm/min; parallel to flow; ASTM D638
Flexural Yield Strength 68.0 MPa9860 psiASTM D790
Flexural Modulus 2.01 GPa292 ksiASTM D790
Izod Impact, Notched 0.390 J/cm0.731 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 123 °C253 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 200 °C356 - 392 °FResin temp
Mold Temperature 40.0 - 80.0 °C104 - 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kolon KOCETAL® CB301 Conductive Grade Acetal Resin

PLAA70 / 49807

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.