MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

3013-H14 Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 3000 Series Aluminum Alloy

Material Notes:

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A93013; Aluminium 3013; AA3013-H14; Al3013-H14
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.74 g/cc0.0990 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 4646
Tensile Strength, Ultimate 155 MPa22500 psi
Tensile Strength, Yield 140 MPa20300 psi0.2% offset
Elongation at Break 9.0 %9.0 %
Modulus of Elasticity 68.9 GPa9990 ksiAA3004 - Average of tension and compression
Poissons Ratio 0.350.35AA3004
Shear Modulus 25.0 GPa3630 ksiAA3004
Shear Strength 90.0 MPa13100 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000416 ohm-cm0.00000416 ohm-cmAA3004
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.2 µm/m-°C
@Temperature 20.0 - 100 °C
12.9 µin/in-°F
@Temperature 68.0 - 212 °F
AA3004
Specific Heat Capacity 0.893 J/g-°C0.213 BTU/lb-°FAA3004
Thermal Conductivity 163 W/m-K1130 BTU-in/hr-ft²-°FAA3004
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 94.7 - 98.4 %94.7 - 98.4 %As remainder
Copper, Cu <= 0.50 %<= 0.50 %
Iron, Fe <= 1.0 %<= 1.0 %
Magnesium, Mg 0.20 - 0.60 %0.20 - 0.60 %
Manganese, Mn 0.90 - 1.4 %0.90 - 1.4 %
Other, each <= 0.050 %<= 0.050 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.60 %<= 0.60 %
Zinc, Zn 0.50 - 1.0 %0.50 - 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3013-O Aluminum
Aluminum 3005-H14
Aluminum 2011-T8
Aluminum 3003-H14
Alclad Aluminum 3003-H12

MA3013H14 / 130352

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.