MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makroblend® UT235 M PC+PET
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend

Material Notes: (PC+PET)-blend, mineral filled, easy flow, low coefficient of linear thermal expansion, easy release, injection molding. Molded parts from UT235M having exceptional dimensional stability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62
Water Absorption at Saturation 0.40 %0.40 %ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0060 cm/cm0.0050 - 0.0060 in/in150x105x3 mm; 270 °C / MT 70°C; 600 bar; b.o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0050 - 0.0060 cm/cm0.0050 - 0.0060 in/in150x105x3 mm; 270 °C / MT 70°C; 600 bar; b.o. ISO 2577
Melt Flow 43 g/10 min
@Load 5.00 kg,
Temperature 270 °C
43 g/10 min
@Load 11.0 lb,
Temperature 518 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 67.0 MPa9720 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 68.0 MPa9860 psi50 mm/min; ISO 527-1,-2
Elongation at Yield 3.5 %3.5 %50 mm/min; ISO 527-1,-2
Tensile Modulus 4.50 GPa653 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 115 MPa16700 psi2 mm/min; ISO 178
Flexural Yield Strength 110 MPa
@Strain 3.5 %
16000 psi
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 4.65 GPa674 ksi2 mm/min; ISO 178
Flexural Strain at Yield 5.0 %5.0 %2 mm/min; ISO 178
Izod Impact, Unnotched (ISO)  85.0 kJ/m²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
ISO 180-U
 85.0 kJ/m²
@Temperature -30.0 °C
40.4 ft-lb/in²
@Temperature -22.0 °F
ISO 180-U
Charpy Impact Unnotched  8.50 J/cm²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
 8.50 J/cm²
@Temperature -30.0 °C
40.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
Impact 45004500[N], Puncture Max Force; ISO 6603-2
Puncture Energy 36.0 J26.6 ft-lbISO 6603-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 45.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
25.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 45.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
25.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 128 °C262 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 114 °C237 °FISO 75-1,-2
Vicat Softening Point 139 °C
@Load 5.10 kg
282 °F
@Load 11.2 lb
120°C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 °C518 °FISO 294
Mold Temperature 70.0 °C158 °FISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makroblend® AR205 PC+PET
Covestro Makroblend® UT250 HR PC+PET
Covestro Makroblend® UT203 PC+PET
Covestro Makroblend® KU 2-7609 Polycarbonate + PBT, Mineral Filled Impact Grade
Covestro Makrolon® 2807 Polycarbonate, Injection Grade

PCOVEST0800 / 202583

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.