System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Envalior Akulon® F130-C3 PA6
Categories:
Polymer
;
Film
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Film Grade
Material Notes:
Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated
Former DSM Engineering Plastics product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.13
g/cc
0.0408
lb/in³
ISO 1183
Water Vapor Transmission
35.0
g/m²/day
@Temperature 23.0 °C
2.25
g/100 in²/day
@Temperature 73.4 °F
at 85% r.h., film; DIS 15106-1/-3
Oxygen Transmission
1.30
cc-mm/m²-24hr-atm
@Temperature 23.0 °C
3.30
cc-mil/100 in²-24hr-atm
@Temperature 73.4 °F
at 0% r.h., film; DIS 15105-1/-2
1.90
cc-mm/m²-24hr-atm
@Temperature 23.0 °C
4.83
cc-mil/100 in²-24hr-atm
@Temperature 73.4 °F
at 85% r.h., film; DIS 15105-1/-2
Viscosity
810000
cP
@Temperature 260 °C
810000
cP
@Temperature 500 °F
Melt Viscosity; DSM method
300000
cP
@Shear Rate 1000 1/s,
Temperature 280 °C
300000
cP
@Shear Rate 1000 1/s,
Temperature 536 °F
350000
cP
@Shear Rate 1000 1/s,
Temperature 260 °C
350000
cP
@Shear Rate 1000 1/s,
Temperature 500 °F
400000
cP
@Shear Rate 1000 1/s,
Temperature 240 °C
400000
cP
@Shear Rate 1000 1/s,
Temperature 464 °F
600000
cP
@Shear Rate 0.1 1/s,
Temperature 280 °C
600000
cP
@Shear Rate 0.1 1/s,
Temperature 536 °F
800000
cP
@Shear Rate 0.1 1/s,
Temperature 260 °C
800000
cP
@Shear Rate 0.1 1/s,
Temperature 500 °F
1.05e+6
cP
@Shear Rate 0.1 1/s,
Temperature 240 °C
1.05e+6
cP
@Shear Rate 0.1 1/s,
Temperature 464 °F
Viscosity Measurement
3.03
3.03
RSV formic acid, 1g/100ml; DSM method
Viscosity Number
196
cm³/g
1.96
dl/g
ISO 307, 1157, 1628
Thickness
50.0
microns
1.97
mil
film
Mechanical Properties
Metric
English
Comments
Film Tensile Strength at Yield, MD
31.0
MPa
4500
psi
parallel; ISO 527-3
Film Elongation at Break, MD
350 %
350 %
parallel; ISO 527-3
Modulus of Elasticity
0.455
GPa
66.0
ksi
film; DSM-Method, 50 mm/min
Coefficient of Friction, Dynamic
1.0
1.0
film; ISO 8295
Coefficient of Friction, Static
1.2
1.2
film; ISO 8295
Tear Strength Test
32
32
Trouser tear resistance, parallel, film; ISO 6383-1
Film Tensile Strength at Break, MD
82.0
MPa
11900
psi
parallel; ISO 527-3
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
90.0
µm/m-°C
50.0
µin/in-°F
ISO 11359-1/-2
Specific Heat Capacity
1.55
J/g-°C
@Temperature 23.0 °C
0.370
BTU/lb-°F
@Temperature 73.4 °F
2.25
J/g-°C
@Temperature 20.0 - 150 °C
0.538
BTU/lb-°F
@Temperature 68.0 - 302 °F
Optical Properties
Metric
English
Comments
Transmission, Visible
83 %
83 %
film; DSM method
Processing Properties
Metric
English
Comments
Processing Temperature
270
°C
518
°F
Extruder Temperature
Die Temperature
270
°C
518
°F
Roll Temperature
110
°C
230
°F
Descriptive Properties
Extrusion Type
Cast Film
Puncture Resistance
1300 J/m
Film (DSM Method)
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Envalior Akulon® F223-D PA6, Dry, Low/Medium Viscosity
Envalior Akulon® F127 PA6
EMS-Grivory Grilon® BS V0 PA6
EMS-Grivory Grilon® BS 23 PA6
EMS-Grivory Grilon® BG-30 S FA PA6-GF30
PDSM9746 / 161367
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.