MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

TIMCAL ENSACO™ 210G Conductive Carbon Black
Categories: Carbon; Carbon Black; Other Engineering Material; Additive/Filler for Polymer

Material Notes: ENSACO™ & SUPER P™ conductive carbon blacks have a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can originate from the interstices between the carbon black particle due to their complex arrangement and from the porosity.

Applications:

  • black pigment
  • UV stabilizer
  • rubber reinforcement

Information provided by TIMCAL

Key Words: CAS Number 1333-86-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.210 g/cc0.00759 lb/in³Pour Density; ASTM D1513
Volatiles <= 0.20 %<= 0.20 %Weight loss during heating between 105 and 950°C; Internal Method 02
Oil Absorption 155 %155 %OAN (Oil Absorption Number) ml/100g; ASTM D2414
Particle Size 45 µm45 µm2 ppm sieve residue; ASTM D1514
pH 8.0 - 118.0 - 11ASTM D1512
Specific Surface Area 55 m²/g55 m²/gBET Nitrogen Surface Area; ASTM D3037
Mooney Viscosity 4444(1+4), EVA/NBR Strippable Compounds
Ash 0.10 %0.10 %ASTM D1506
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 90 - 9490 - 94EVA/NBR Strippable Compounds
Tensile Strength 1.90 - 16.9 MPa276 - 2450 psiEVA/NBR Strippable Compounds
Elongation at Break 130 - 180 %130 - 180 %EVA/NBR Strippable Compounds
100% Modulus 12.2 MPa
@Strain 100 %
1770 psi
@Strain 100 %
EVA/NBR Strippable Compounds
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 500 ohm-cm<= 500 ohm-cm25% carbon black in HDPE; Internal Method 11
 6600 ohm-cm6600 ohm-cmEVA/NBR Strippable Compounds
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 0.10 %0.10 %as packed; ASTM D1509
Sulfur, S <= 0.50 %<= 0.50 %ASTM D1619
 
Descriptive Properties
AspectFine black granules
COAN (Crushed OAN) ml/100g95ASTM D3493
Peel Strength3 Nhot air 100°C, EVA/NBR Strippable Compounds
 3 Nhot air 100°C after 21 days, EVA/NBR Strippable Compounds
 4 Nhot air 100°C after 3 days, EVA/NBR Strippable Compounds
Toluene Extract, Max, %0.1ASTM D4527

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TIMCAL ENSACO™ 250G Conductive Carbon Black Compounds
Graphite, Carbon, C
TIMCAL ENSACO™ 150G Conductive Carbon Black
TIMCAL ENSACO™ 350G Conductive Carbon Black
TIMCAL SUPER P® Li Carbon Black Additive

CTIMCAL01 / 2643

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.