MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem EF2002 Blown Film Extrusion Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade; Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Description: EF2002 is a low-density polyethylene (LDPE) with high molecular weight. Has excellent processability, proper of branched polyethylene produced by a high-pressure process. EF2002 resin presents an excellent performance in conventional LDPE extruders, granting low energy consumption during the whole process and allowing the production of packaging with a good dimensional uniformity and an excellent surface finishing.

Additives: No additives

Application: High resistance films for industrial packaging, heavy duty bags and plastic canvas. Base resin for agriculture films with big dimensions.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
Melt Flow 0.16 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.16 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 360 %360 %ASTM D882
Film Elongation at Break, TD 740 %740 %ASTM D882
Elmendorf Tear Strength MD 180 g180 gASTM D1922
Elmendorf Tear Strength TD 200 g200 gASTM D1922
Dart Drop Test 200 g0.441 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 30.0 MPa4350 psiASTM D882
Film Tensile Strength at Break, TD 25.0 MPa3630 psiASTM D882
1% Secant Modulus, MD 150 MPa21800 psi2% Secant; ASTM D882
1% Secant Modulus, TD 170 MPa24700 psi2% Secant; ASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 19 %19 %ASTM D1003
Gloss 53 %53 %60°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 225 °C338 - 437 °FProfile

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Petroquimica Triunfo Trithene® TX 7001 LDPE - High Molecular Weight

PBRASK2092 / 199973

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.