MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Phosphor Bronze, 5% Sn, UNS C51000, HR04 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: Hard and Stress Relieved

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Butt Weld, Capacity for Being Cold Worked; Good Suitability – Gas Shielded Arc Welding, Spot Weld; Fair Suitability – Oxyacetylene Welding, Coated Metal Arc Welding, Seam Weld; Poor Suitability – Capacity for Being Hot Formed

Common Fabrication Processes: Blanking; Drawing; Forming and Bending; Heading and Upsetting; Roll Threading and Knurling; Shearing; Stamping

Typical uses: Bridge Bearing Plates; Electrical Connectors; Electrical Flexing Contact Blades; Electromechanical Spring Components; Electronic and Precision Instrument Parts; Electronic Connectors; Fuse Clips; Resistance Wire; Switch Parts; Wire Brushes; Cotter Pins; Fasteners; Lock Washers; Beater Bar; Bellows; Bourdon Tubes; Chemical hardware; Clutch Disks; Diaphragms; Perforated Sheets; Pressure Responsive Elements; Sleeve Bushings; Springs; Textile machinery; Truss Wire; Welding Rods

Applicable Specifications: Bar – ASTM B139/B139M, AMS 4625, ASTM B103/B103M; Bearings & Busings – MILITARY MIL-B-13501; Bolts – ASTM F468; Bushing Stock – MILITARY MIL-B-13501; Nuts – ASTM F467; Plate – ASTM B103/B103M, Bridge and Bearing ASTM B100, AMS 4510; Rod – ASTM B139/B139M, SAE J463, AMS 4625, SAE J461; Screws – ASTM F468; Shapes – ASTM B139/B139M; Sheet – SAE J463, AMS 4510, Bridge and Bearing ASTM B100, SAE J461, ASTM B103/B103M; Strip – AMS 4510, SAE J463, ASTM B888/B88M, ASTM B103/B103M, SAE J461; Studs – ASTM F468; Tube – MILITARY MIL-T-3595, AMS 4625; Wire – ASTM B159/B159M, AMS 4720, MILITARY MIL-W-6712, SAE J461, SAE J463

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.86 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 579 MPa84000 psi
Tensile Strength, Yield 510 MPa74000 psi0.2% Offset
Elongation at Break 14 %14 %
Tensile Modulus 110 GPa16000 ksi
Modulus of Rigidity 41.4 GPa6000 ksi
Poissons Ratio 0.330.33Calculated
Machinability 20 %20 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000115 ohm-cm0.0000115 ohm-cm15% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.8 µm/m-°C
@Temperature 20.0 - 300 °C
9.90 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 5.76 W/m-K40.0 BTU-in/hr-ft²-°F
Melting Point 954 - 1050 °C1750 - 1920 °F
Solidus 954 °C1750 °F
Liquidus 1050 °C1920 °F
Annealing Point 482 - 677 °C900 - 1250 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 93.4 - 95.8 %93.4 - 95.8 %As Balance
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.050 %<= 0.050 %
Phosphorus, P 0.030 - 0.35 %0.030 - 0.35 %
Tin, Sn 4.2 - 5.8 %4.2 - 5.8 %
Zinc, Zn <= 0.30 %<= 0.30 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC51000x5 / 292995

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.