MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mocom (ALBIS) TEDUR® L 9412-3.2 Polyphenylene Sulphide, 10% PTFE, 10% Carbon Fibers, 10% Graphite Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler

Material Notes: Base Polymer: Polyphenylene Sulphide

Filler/Additive System: 10% PTFE, 10% Carbon Fibers, 10% graphite

Special Features: Reduced surface resistivity, electrically conductive, improved sliding/wear

Market Segment: Automotive, Machinery, Electrical and Electronic

Typical Applications: Bearings and sliding elements, functional components, housings

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ISO 1183
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psiISO 527
Elongation at Break 1.3 %1.3 %ISO 527
 1.7 %1.7 %deflection at max force; ISO 178
Tensile Modulus 13.6 GPa1970 ksiISO 527
Flexural Strength 180 MPa26100 psiISO 178
Flexural Modulus 11.9 GPa1730 ksiISO 178
Izod Impact, Unnotched (ISO) 20.0 kJ/m²9.52 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 150 ohm<= 150 ohmDIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 272 °C522 °FISO 75-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 320 - 340 °C608 - 644 °FInjection molding
Mold Temperature >= 140 °C>= 284 °FInjection molding
Drying Temperature 130 - 140 °C
@Time 7200 - 14400 sec
266 - 284 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerPolyphenylene Sulfide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALBIS8933 / 242992

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.