MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arya Sasol LFI 2447A Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Product Description: LFI2447A is a low density polyethylene, with good toughness and good optical properties. This product offers a high level of antiblock and slip agent (Erucamide), low energy consumption during processing and a good draw down ability. It typically exhibits low friction and low blocking. LFI2447A has been manufactured under SABTEC licensed technology

Application: Blown film extrusion, high clarity laundry bag, textile wrapping film, zip lock bag

Forms: Pellets

Attribute: Good toughness, good optical properties, high speed converting without sticking

Additives: Antioxidant: Yes; Antiblock: Yes; Slip Agent: Yes

Information provided by

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ISO 1183
Thickness 25.0 - 50.0 microns0.984 - 1.97 mil
Melt Flow 4.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.7 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 13.0 MPa1890 psiISO 527-1,3
Film Tensile Strength at Yield, TD 13.0 MPa1890 psiISO 527-1,3
Film Elongation at Break, MD >= 100 %>= 100 %ISO 527-1,3
Film Elongation at Break, TD >= 450 %>= 450 %ISO 527-1,3
Modulus of Elasticity 0.250 GPa36.3 ksiTD; ISO 527-1,3
 0.350 GPa50.8 ksiMD; ISO 527-1,3
Coefficient of Friction 0.200.20ASTM D1894
Tear Strength 30.0 kN/m171 pliTD; ISO 6383-2
 90.0 kN/m514 pliMD; ISO 6383-2
Dart Drop Total Energy 13.0 J/cm0.0244 ft-lb/milASTM D4272
Film Tensile Strength at Break, MD 27.0 MPa3920 psiISO 527-1,3
Film Tensile Strength at Break, TD 16.0 MPa2320 psiISO 527-1,3
 
Optical PropertiesMetricEnglishComments
Haze 9.0 %9.0 %ASTM D1003 A
Gloss 55 %55 %[GU], 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 145 - 160 °C293 - 320 °FExtruder temperature profile
Blow-up Ratio (BUR) 2.0 - 3.02.0 - 3.0
 
Descriptive Properties
Blocking<5 gASTM D3354
Clarity28 mVSABTEC method
Re-blocking20 gSABTEC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARYA007 / 250461

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.