MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Borealis Fibremod™ GF027SFB Polypropylene, Chemically Coupled Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Fibremod™ GF027SFB is a chemically coupled glass fiber reinforced polypropylene compound intended for injection molding.

Applications: Fibremod GF027SFB has been developed especially for demanding applications in the automotive industry.

  • Structural parts
  • Complex custom parts
Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 95° - 105°C.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ISO 1183
Melt Flow 18.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
18.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature <= 50.0 °C<= 122 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 34.0 MPa4930 psi50 mm/min; ISO 527-2
Flexural Modulus 1.65 GPa239 ksi2 mm/min; ISO 178
 
Processing PropertiesMetricEnglishComments
Feed Temperature 230 - 280 °C446 - 536 °F
Mold Temperature 20.0 - 50.0 °C68.0 - 122 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9769 / 323126

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.