MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Vamac® VMX5015 65-70 Shore A Ethylene Methacrylate (AEM)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: Pre-Compound for Improved Heat Resistance

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Mooney Viscosity  56
@Temperature 100 °C
56
@Temperature 212 °F
ML 1+4, Compound; ISO 289-1-2
 57
@Temperature 100 °C
57
@Temperature 212 °F
ML 1+4; ISO 289-1-2
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 66663s; ISO 48-4
Tensile Stress at Strain 5.80 MPa
@Strain 100 %
841 psi
@Strain 100 %
ISO 527-1/-2
Tear Strength 2.60 kN/m14.8 pliparallel; ISO 34-1
Compression Set 23 %
@Temperature 150 °C,
Time 252000 sec
23 %
@Temperature 302 °F,
Time 70.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 185 °C365 °FDuPont proprietary test
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 °C
@Time 14400 sec
347 °F
@Time 4.00 hour
Cure Time 10.0 min
@Temperature 180 °C
0.167 hour
@Temperature 356 °F
 
Descriptive Properties
Colorcolor may variate between white and pink
Moving Die Rheometer at 180°C (minutes)2.6t(50); ISO 6502
 7.3t(90); ISO 6502
Moving Die Rheometer at 180°C (N mm)69-1500torque; ISO 6502
Polymer(AEM)
Scorch, Mooney viscosity> 41MS at 121°C; ISO 289-1-2
Scorch, time to 10 unit rise17MS at 121°C; ISO 289-1-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX4621 / 265831

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.