MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Celanese CoolPoly® D5506 Thermally Conductive Liquid Crystalline Polymer
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes: CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows design freedom in applications previously restricted to metals. The D series is electrically non-conductive and can be used for its dielectric properties.

CoolPoly D5506 is a thermally conductive injection molding resin based on a liquid crystal polymer matrix. CoolPoly D5506 is electrically insulative. Thermally conductive polymers like CoolPoly D5506 cool faster than standard injection molding grade resins.

Information provided by Cool Polymers, Inc.

Celanese acquired Cool Polymers in 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³ISO 1183
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inASTM D551
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 55.0 MPa7980 psiISO 527-1
Elongation at Break 0.76 %0.76 %ISO 527-1
Tensile Modulus 10.7 GPa1550 ksiISO 527-1
Flexural Strength 84.0 MPa12200 psiISO 178
Flexural Modulus 12.7 GPa1840 ksiISO 178
Charpy Impact Unnotched 0.560 J/cm²2.67 ft-lb/in²ISO 179-1
Charpy Impact, Notched 0.280 J/cm²1.33 ft-lb/in²ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.60e+16 ohm-cm1.60e+16 ohm-cmASTM D257
Surface Resistivity per Square 2.00e+14 ohm2.00e+14 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 6.40 µm/m-°C
@Temperature 20.0 °C
3.56 µin/in-°F
@Temperature 68.0 °F
ASTM E831-03
CTE, linear, Transverse to Flow 11.3 µm/m-°C
@Temperature 20.0 °C
6.28 µin/in-°F
@Temperature 68.0 °F
ASTM E831-03
Specific Heat Capacity 0.970 J/g-°C0.232 BTU/lb-°FASTM E1461
Thermal Conductivity 10.0 W/m-K69.4 BTU-in/hr-ft²-°FASTM E1461
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C>= 572 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 264 °C507 °FISO 75-1/-2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 330 - 360 °C626 - 680 °F
Middle Barrel Temperature 340 - 370 °C644 - 698 °F
Front Barrel Temperature 345 - 380 °C653 - 716 °F
Nozzle Temperature 350 - 382 °C662 - 720 °F
Melt Temperature 349 - 393 °C660 - 739 °F
Mold Temperature 93.0 - 177 °C199 - 351 °F
Drying Temperature 180 °C356 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content 0.010 %0.010 %
Dew Point -34.0 °C-29.2 °F
Injection Pressure 35.0 - 70.0 MPa5080 - 10200 psi
Hold Pressure 7.00 - 35.0 MPa1020 - 5080 psi
Back Pressure 0.000 - 0.350 MPa0.000 - 50.8 psi
Screw Speed 75 - 150 rpm75 - 150 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese CoolPoly® D5502 Thermally Conductive Liquid Crystalline Polymer
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Celanese CoolPoly® E2 Thermally Conductive Liquid Crystalline Polymer
Avient Therma-Tech™ LC-5000C TC LCP
Celanese CoolPoly® D5110 Thermally Conductive Polyphenylene Sulfide

PCOOL19 / 29015

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.