MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman FORMION™ FI 241E Non-Reinforced, Extrusion Grade Ionomer Alloy
Categories: Polymer; Thermoplastic; Ionomer

Material Notes: Description

Formion® FI 241E is a patented non-reinforced, extrusion grade Ionomer alloy. It has bee formulated for high durability, low gloss, and low temperature ductility.
Application

Formion® FI 241E is targeted for exterior or interior appearance or packaging applications in film, blow molding, thermoforming or extrusion applications, which may require low tack, low gloss, and excellent colorability.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccISO 1183/1
Linear Mold Shrinkage 0.011 - 0.019 cm/cm
@Thickness 3.20 mm
0.011 - 0.019 in/in
@Thickness 0.126 in
72 hr; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 454515 sec delay; ISO 868
Tensile Strength, Ultimate 9.50 MPa1380 psiat max load; ISO 527
Elongation at Break 165 %165 %ISO 527
Flexural Modulus 0.109 GPa15.8 ksiTangent; ISO 178
Izod Impact, Notched (ISO) NBNBISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 36.0 °C
@Thickness 3.20 mm
96.8 °F
@Thickness 0.126 in
ISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman FORMION™ FI 234 20% Mineral Reinforced Ionomer / Nylon Alloy
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy
Dow Surlyn® 2601B Sodium Ionomer
Dow Surlyn® 6320 Magnesium Ionomer
Dow Surlyn® 7930 Ionomer Resin, Lithium

PASHU031 / 24995

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.