MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Bakelite® Keripol® RW 1411 Polyester Molding Compound, Low Shrinkage, Resistant to High Temperatures
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Polyester molding compound, inorganically filled glass fiber reinforced, styrene free, tracking resistance 600 V, good heat resistance, high viscosity flow characteristics.

Applications: H4 and H7 lamp sockets.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.15 g/cc0.0777 lb/in³ISO 1183
Apparent Bulk Density 1.00 g/cc0.0361 lb/in³ISO 60
Linear Mold Shrinkage 0.0015 cm/cm0.0015 in/inCompression Molding. Post Shrinkage = -0.03%.; ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 85.0 MPa12300 psiISO 178
Flexural Modulus 17.0 GPa2470 ksiISO 178
Charpy Impact Unnotched 0.500 J/cm²2.38 ft-lb/in²ISO 179-1 eU
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm
Surface Resistance 1.00e+12 ohm1.00e+12 ohm
Dielectric Constant 6.0
@Frequency 100 Hz
6.0
@Frequency 100 Hz
Dielectric Strength 30.0 kV/mm
@Thickness 1.00 mm
762 kV/in
@Thickness 0.0394 in
IEC 60243-P1
Dissipation Factor 0.0080
@Frequency 100 Hz
0.0080
@Frequency 100 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 8.0 MPa 160 °C320 °FISO 75-2
 
Descriptive Properties
Water absorption (mg)1524h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bakelite® Keripol® RFT 1221 Polyester Molding Compound, Low Coefficient of Friction, High Surface Quality, Low Shrinkage, UL Listed
Evonik Vestodur® GF20-FR5 20% Glass Reinforced, Flame Retardant PBT
Evonik Vestoran® 1300-GF20 nf PPE
A. Schulman BMC 1000 Thermoset Polyester, Food Grade
A. Schulman BMC 100 Thermoset Polyester, GP

PBAKE059 / 27093

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.