MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil SpectraSyn™ 40 Polyalphaolefin (PAO) Fluid
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Product Description: SpectraSyn™ High Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties (pour point and viscosity), low volatility, and improved thermal stability. SpectraSyn™ High Viscosity (PAO) products have high viscosity indices translate into improved flow at low temperatures and increased film thickness at high temperatures. SpectraSyn™ High Viscosity PAO basestocks are particularly suited for industrial oils requiring high stability under extreme operating conditions. SpectraSyn™ High Viscosity PAO products are frequently used in conjunction with lower viscosity fluids (PAO, mineral oils) as a viscosity booster to achieve a wide range of ISO VG industrial and automotive gear oils.

Appearance: Bright & Clear

Availability: Africa & Middle East, Asia Pacific, Central America, Europe, North America and South America

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.850 g/cc
@Temperature 15.6 °C
0.0307 lb/in³
@Temperature 60.1 °F
ASTM D4052
Brookfield Viscosity 102000 cP
@Temperature -26.0 °C
102000 cP
@Temperature -14.8 °F
ASTM D2983
Viscosity Measurement 147147Index; ASTM D2270
Kinematic Viscosity  4840 cSt
@Temperature 0.000 °C
4840 cSt
@Temperature 32.0 °F
ASTM D445
 40500 cSt
@Temperature -20.0 °C
40500 cSt
@Temperature -4.00 °F
ASTM D445
Kinematic Viscosity at 40°C (104°F) 396 cSt396 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 39 cSt39 cStASTM D445
Vapor Pressure 0.00120 bar
@Temperature 200 °C
0.900 torr
@Temperature 392 °F
ASTM D2879
Evaporation Loss  0.40 %
@Temperature 150 °C,
Time 79200 sec
0.40 %
@Temperature 302 °F,
Time 22.0 hour
ASTM D972
 2.5 %
@Temperature 205 °C,
Time 23400 sec
2.5 %
@Temperature 401 °F,
Time 6.50 hour
ASTM D972
Surface Tension 38.9 dynes/cm38.9 dynes/cmASTM D1331A
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.10<= 0.10[mg KOH/g]; ASTM D974 (mod)
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.152.15ASTM D924
Dielectric Breakdown 38900 V38900 V
 
Thermal PropertiesMetricEnglishComments
Pour Point -36.1 °C-33.0 °FASTM D5950/D97
Flash Point 281 °C538 °FCOC; ASTM D92
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4681.468ASTM D1218
 
Descriptive Properties
Aniline Point319.3°FASTM D611
Color<0.5ASTM D1500
CompositionWater<50 ppm, ASTM D6304 (mod)
Density Correction Factor0.000605 (g/cc)/°CASTM D1250
Fire Point604°FCOC, ASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil SpectraSyn™ 100 Polyalphaolefin (PAO) Fluid
ExxonMobil SpectraSyn™ 10 Polyalphaolefin (PAO) Fluid

PEX99688 / 175924

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.