MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zircar Zirconia ZYBF-3 Zirconia Bulk Fiber Insulation
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Zirconia Bulk Fibers Type ZYBF are yttria stabilized zirconia fibers available in five different forms, all having useful properties up to 2200°C. These polycrystalline fibers can be vacuum formed into rigid shapes, placed into cavities as loose fill insulation, or added to ceramic bodies and coatings for reinforcement. They are differentiated by fiber length, surface area, crystallite size and porosity. However, they all share the same fiber diameter and calcined chemical composition. All five forms of ZYBF are made using the “Zircar Process” which replicates the gross physical structure of an organic precursor fiber with a ceramic. Typically these fibers are 6 to10 microns in diameter and have a serrated outside surface.

All of our Zirconia Bulk Fibers are phase stabilized with ~10% yttria (yttrium oxide - Y2O3) to maintain a stable tetragonal / cubic structure. The yttria, in a solid solution within the zirconia, stabilizes the tetragonal / cubic structure by preventing the monoclinic to tetragonal crystal transformation that occurs at 1170°C in pure un-stabilized or insufficiently stabilized zirconia. This undesirable transformation causes an 11% volume change in the crystal unit cell size that can cause micro-cracking and reduced physical strength in the bulk solid.

Yttria stabilized zirconia is an electrical semiconductor at elevated temperatures. This conductivity arises from the different valences of ionic Zr+4 and Y+3. Electricity is conducted at elevated temperatures (~700-800°C) as oxygen ions are induced to flow through the stabilized zirconia structure. This phenomenon forms the basis of zirconia oxygen sensors.

Features:

  • Available in Five Different Forms
  • Low Thermal Conductivity
  • Highly Refractory
  • Low Heat Storage
  • Extreme High Temperature Stability
  • Fibers Stabilized with ~10 wt% Yttria
  • Lightweight
  • Available “Off the Shelf”

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.420 g/cc0.0152 lb/in³
Loss On Ignition 0.10 - 0.40 %
@Temperature 950 °C,
Time 1800 sec
0.10 - 0.40 %
@Temperature 1740 °F,
Time 0.500 hour
Specific Surface Area 0.40 m²/g0.40 m²/g
Pore Size 0.00360 microns0.000142 milMedian Pierce desorption mesopore, based on surface area
 0.00430 microns0.000169 milMedian Pierce adsorption mesopore, based on surface area
 0.0280 microns0.00110 milMedian Pierce desorption mesopore, based on pore volume
 0.170 microns0.00669 milMedian Pierce adsorption mesopore, based on pore volume
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl <= 0.10 %<= 0.10 %
H2O, Water 0.050 - 0.20 %0.050 - 0.20 %
HfO2 1.0 - 2.0 %1.0 - 2.0 %
Y2O3 10 %10 %
ZrO2 88 - 89 %88 - 89 %
 
Descriptive Properties
Trace Impurities<1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Zirconia ZYBF-1 Zirconia Bulk Fiber Insulation
Titanium Nitride (TiN) Coating
Zoltek™ PX35YZ0106 Carbon Fiber Yarn
Goodfellow Alumina Silicate SiO2 53/Al2O3 47
DowAksa AKSACA™ A-38 6K Continuous Carbon Fiber

C6ZIR023 / 2779

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.