MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epichlorohydrin Rubber (CO, ECO)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: CO is the ISO designation for the homopolymer and ECO is the ISO designation for the ethylene oxide copolymer. Epichlorohydrin rubber is generally damaged by chlorinated solvents, ketones, aldehydes, esters, and nitrogen-containing solvents. It is generally resistant to oil/fat/grease, ozone, and hydraulic fluid.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 - 1.60 g/cc0.0524 - 0.0578 lb/in³Compounded
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 40 - 9040 - 90Depends on compounding
Tensile Strength, Ultimate 17.0 MPa2470 psiCompounded Tire
Elongation at Break 150 - 500 %150 - 500 %
Compression Set 10 %10 %
 
Thermal PropertiesMetricEnglishComments
CTE, linear 648 µm/m-°C
@Temperature 20.0 °C
360 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -40.0 - -10.0 °C-40.0 - 14.0 °F

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Propylene Oxide Rubber (GPO)
Ethylene Propylene Rubber (EPM, EPDM)
Trelleborg P650 Epichlorohydrin
Chlorosulfonated Polyethylene Rubber (CM, CSM)
Fluorocarbon Rubber (FPM), Low Temperature Grade

P0RU10 / 20058

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.